Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 40.0 GPa | 5800 ksi | ASTM D790 |
Hexcel® HexMC™ C / 2000 / R1 Composite SMC High performance sheet-molding compound, specifically designed for compression molding. The epoxy matrix and high carbon fiber volume enable components to be molded for a wide range of applications.. |
|||
Flexural Modulus | 40.0 GPa | 5800 ksi | ASTM D4476 |
Dow Fulcrum™ Thermoplastic Glass-Filled Polyurethane Composite Rod FULCRUM Thermoplastic Composite Technology is specifically designed for the fabrication of continuous fiber composites that have greater flexibility in post-processing operations as well as higher t.. |
|||
Flexural Modulus | 40.0 GPa | 5800 ksi | transverse; ISO 178 |
Bond Laminates TEPEX® dynalite 408-C200(2)-FG290(2)/45% Carbon – Filament Glass – TPU Consolidated Composite Laminate Within the TEPEX® composite laminate, TPU distinguishes itself from alternative resin systems by its specific physical properties. The TPU resin is tough which results in an excellent impact and f.. |