Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.93 GPa | 570 ksi | ASTM D790 |
PolyOne LubriOne™ NY-10GF/10T BLACK Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Flexural Modulus | 3.93 GPa | 570 ksi | ASTM D790 |
Polymer Resources TP-G10 Polybutylene Terephthalate, 10% Glass Reinforced Polybutylene Terephthalate, 10% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information prov.. |
|||
Flexural Modulus | 3.93 GPa | 570 ksi | 1.3 mm/min; ASTM D790 |
PolyOne Edgetek® AS-10GF/000 BLACK Acrylonitrile Butadiene Styrene (ABS) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Flexural Modulus | 3.93 GPa | 570 ksi | ASTM D790 |
PolyOne Edgetek® AS-03CF/000 Acrylonitrile Butadiene Styrene (ABS), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 3.93 GPa | 570 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics REMEX VR4831 PBT 15% Glass filled PBT, Flame retardant, UL Recognized, Utility grade, Black color only |
|||
Flexural Modulus | 3.93 GPa | 570 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP RAL23 PA 66 LNP LUBRICOMP* RAL23 is a compound based on Nylon 66 resin containing 15% PTFE, 10% Aramid Fiber. Added features of this material include: Wear Resistant. |
|||
Flexural Modulus | 3.93 GPa | 570 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP RAL23 PA 66 (Asia Pacific) LNP LUBRICOMP* RAL23 is a compound based on Nylon 66 resin containing Aramid Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 3.93 GPa | 570 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP RAL23 PA 66 (Europe-Africa-Middle East) LNP LUBRICOMP* RAL23 is a compound based on Nylon 66 resin containing PTFE, Aramid Fiber. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 3.93 GPa | 570 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP RAL23S PA 66 LNP LUBRICOMP* RAL23S is a compound based on Nylon 66 resin containing 10% PTFE, 15% Aramid. Added features of this material include: Heat Stabilized, Wear Resistant. |
|||
Flexural Modulus | 3.93 GPa | 570 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP RAL23S PA 66 (Asia Pacific) LNP LUBRICOMP* RAL23S is a compound based on Nylon 66 resin containing Aramid Fiber, PTFE. Added features of this material include: Heat Stabilized. |
|||
Flexural Modulus | 3.93 GPa | 570 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP RAL23S PA 66 (Europe-Africa-Middle East) LNP LUBRICOMP* RAL23S is a compound based on Nylon 66 resin containing PTFE, Aramid Fiber. Added features of this material include: Heat Stabilized. |
|||
Flexural Modulus | 3.93 GPa | 570 ksi | ASTM D790 |
Techmer ES Electrablend® PC 04008 FR BK Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI) and Flame RetardantAppearance: BlackInformation provided by TP Composite.. |
|||
Flexural Modulus | 3.93 GPa | 570 ksi | ASTM D790 |
Techmer ES Electrablend® PC 04009 FR BK Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI) and Flame RetardantAppearance: BlackInformation provided by TP Composite.. |
|||
Flexural Modulus | 3.93 GPa | 570 ksi | ASTM D790 |
Techmer ES HiFill® ABS WM20 20% Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 20% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 3.93 GPa | 570 ksi | ASTM D790 |
Techmer ES HiFill® ABS IM TM20 20% Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 20% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedProcessing Method: Injection MoldingInformation p.. |
|||
Flexural Modulus | 3.93 GPa | 570 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP MF003AS PP LNP* THERMOCOMP* MF003AS is a compound based on Polypropylene containing 15% Glass Fiber. Characteristics of this grade are: Heat Stabilized. |
|||
Flexural Modulus | 3.93 GPa | 570 ksi | Tangent; ASTM D790 |
Plastics Group Polifil® GFPC-10 10% Glass-Reinforced Polycarbonate Polifil® GFPC series compounds offer a combination of improved dimensional stability and decreased flammability. The excellent balance of physical properties make the Polifil® glass-filled polycar.. |
|||
Flexural Modulus | 3.93 GPa | 570 ksi | ASTM D790 |
Clariant Renol PCSP0017 Polycarbonate/Polyester Alloy, 30% Glass Reinforced Data provided by Clariant Masterbatches |
|||
Flexural Modulus | 3.93 GPa | 570 ksi | ASTM D790 |
Asahi Kasei Thermylene® P6-20FG-0693 20% Glass Fiber Reinforced, Heat and UV Stabilized Information provided by Asahi Thermofil |
|||
Flexural Modulus | 3.93 GPa | 570 ksi | ASTM D790 |
Asahi Kasei Thermylene® P6-23FG-2600 23% Glass Fiber Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Flexural Modulus | 3.93 GPa | 570 ksi | ASTM D790 |
Asahi Kasei Thermofil D-10FG-1101 10% Glass Fiber Reinforced, ABS Information provided by Asahi Thermofil |
|||
Flexural Modulus | 3.93 GPa | 570 ksi | ASTM D790 |
PlastxWorld CEVIAN® A2604 20% GF PA/ABS Alloy, Conditioned Property data is for samples at equilibrium moisture (1.1%)These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWo.. |