Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.72 GPa | 540 ksi | ASTM D790 |
PolyOne Maxxam™ PD 40 TF Black Polypropylene Homopolymer (PP Homopolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Flexural Modulus | 3.72 GPa | 540 ksi | ASTM D790 |
PolyOne Nymax™ GB 1200 30 HS BLACK 18 Polyamide 66 (Nylon 66) Preliminary Data SheetMolded Test Bars: Dry as MoldedInformation provided by PolyOne |
|||
Flexural Modulus | 3.72 GPa | 540 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Cycolac® INP564 ABS SABIC INP564 provides compatibility with a wider range of ABS grades than many color concentrate bases; allows better dispersion than pellets; allows concentrate manufacturers to produce both pellet.. |
|||
Flexural Modulus | 3.72 GPa | 540 ksi | ASTM D790 |
Polymer Resources PPX-FRG10 Modified-PPO, V-1 Flame Retardant, 10% Glass Reinforced Modified-Polyphenylene Oxide, V-1 Flame Retardant, 10% Glass ReinforcedFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing condu.. |
|||
Flexural Modulus | 3.72 GPa | 540 ksi | ASTM D790 |
Multibase Multi-Pro® 4005 MI Polypropylene Mica Filled, 40% by weight.Features:Rigidity, HighImpact Resistance, GoodForms:PelletsProcessing Methods:Injection MoldingUses:Automotive ApplicationsInformation provided by Multibase |
|||
Flexural Modulus | 3.72 GPa | 540 ksi | ASTM D790 |
Polymer Resources NY66-IMG13 Nylon, 13% Glass Reinforced, Impact Modified (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Flexural Modulus | 3.73 GPa @Thickness 3.20 mm |
540 ksi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOS GP2100 ABS+GF10%, General Purpose Feature: Injection Molding, ABS+GF10%, General PurposeApplication: Electric & Electronic (Housing, Components)CAS No. 9003-56-9, 9003-54-7 and 65997-17-3Information provided by LG Chemical |
|||
Flexural Modulus | 3.73 GPa @Thickness 3.20 mm |
540 ksi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
LG Chemical Lupox® GP2056F PBT+GF5% Description: Injection Molding, PBT+GF5%, Flame Retardant Application: IT/OA, E&E (Connector)CAS No. 71342-77-3, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chemical |
|||
Flexural Modulus | 3.73 GPa @Temperature 23.0 °C |
540 ksi @Temperature 73.4 °F |
ASTM D790 |
IRPC Polimaxx Polene 121PC Styrene Acrylonitrile APPLICATIONS: INJECTION MOLDING, HOUSEHOLD PRODUCTS : SANITARY WARE, AUTOPART APPLICATION : LAMP ELECTRICAL APPLIANCES : ELECTRICAL FAN |
|||
Flexural Modulus | 3.73 GPa @Temperature 23.0 °C |
540 ksi @Temperature 73.4 °F |
ASTM D790 |
IRPC Polimaxx Polene 330PC Styrene Acrylonitrile APPLICATIONS: INJECTION MOLDING, HOUSEHOLD PRODUCTS : SANITARY WARE, AUTOPART APPLICATION : LAMP ELECTRICAL APPLIANCES : ELECTRICAL FAN |
|||
Flexural Modulus | 3.72 GPa | 540 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP KFP032 Acetal Copolymer (Asia Pacific) LNP* LUBRICOMP* KFP032 is a compound based on Acetal Copolymer resin containing PTFE, Silicone, Glass Fiber. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 3.72 GPa | 540 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM 1100 PEI (Asia Pacific) Standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0, V2 and 5VA listing. |
|||
Flexural Modulus | 3.72 GPa | 540 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Ultem 1100EF PEI Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, U.S. FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 3.72 GPa | 540 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Ultem 1100EF PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, U.S. FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 3.72 GPa | 540 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Ultem 1100EF PEI (Europe-Africa-Middle East) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, U.S. FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.. |
|||
Flexural Modulus | 3.72 GPa | 540 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM 1100F PEI (Asia Pacific) Standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0, V2 and 5VA listing. US FDA and EU Food Contact compliant. Effective June 2007, this grade will no longer be supported with biocompati.. |
|||
Flexural Modulus | 3.72 GPa | 540 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM 1110 PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C). ECO Conforming. |
|||
Flexural Modulus | 3.72 GPa | 540 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Ultem 1110R PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 3.72 GPa | 540 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Ultem 1110V PEI (Europe-Africa-Middle East) Enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Modulus | 3.72 GPa | 540 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRILOY UA200A PPA (Asia Pacific) LNP LUBRILOY* UA200A is a compound based on Polyphthalamide resin containing Aramid Fiber, Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 3.72 GPa | 540 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM HU1110 PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contac.. |
|||
Flexural Modulus | 3.72 GPa | 540 ksi | 2.6 mm/min, 100 mm span; ASTM D 790 |
SABIC Innovative Plastics Ultem MD130A PEI Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming. US FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 3.72 GPa | 540 ksi | tangent; ASTM D790 |
Spartech EP5140 Talc Filled Homopolymer Provides the highest level of stiffness and heat resistance of filled olefins. Talc filled grades offer the highest strength properties. Typical applications include extrusion/thermoformed food cont.. |
|||
Flexural Modulus | 3.72 GPa | 540 ksi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF12 TL20 12% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 12% Filler by Weight Additive: Heat Stabilizer and PTFE Lubricant(20%)Features: Lubricated and Heat Stabiliz.. |
|||
Flexural Modulus | 3.73 GPa | 540 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® LS-3104G PC, 10% Glass Filled High Impact High-impact resistant PC/GF with 10% GF reinforcement for LCD BLFInformation provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 3.73 GPa | 540 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® NH-1150HH PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 3.72 GPa | 540 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Ultem 1110V PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 3.72 GPa | 540 ksi | ASTM D790 |
Teknor Apex Chemlon® 109-18 GH Nylon 66, 18% Glass Fiber Reinforced Notes: High-impact; Reinforced with 18% glass fibers; Highly toughened compound designed to improve practical toughness and ductility Features: Ductile; Good Impact Resistance; Good Toughness; Good .. |
|||
Flexural Modulus | 3.72 GPa | 540 ksi | ASTM D790 |
SABIC Innovative Plastics NORYL PX2907 PPE+PS (Asia Pacific) PPE+HIPS GF10% FR V-1 |
|||
Flexural Modulus | 3.72 GPa | 540 ksi | ASTM D790 |
PlastxWorld CEVIAN®-N 080 SAN resin These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |