Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.70 GPa | 537 ksi | |
Plastcom SLOVALEN PH 72 T 40 PP, 40% mineral filling FeaturesModified homopolymer PP for injection moulding with the content of 40% microground, floated, thermo stable, chemically modified talc. General application in all industry branches - covers of.. |
|||
Flexural Modulus | 3.70 GPa | 537 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycolac® INPBMAT ABS Cross-linked SAN in styrenic matrix. Provides excellent gloss reduction properties. Maintains original polymer properties such as impact etc. Compatible with various polymer such as PVC and ABS. C.. |
|||
Flexural Modulus | 3.70 GPa @Temperature 23.0 °C |
537 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYfill PPH T8038 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Modulus | 3.70 GPa @Temperature 23.0 °C |
537 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYsan PN127 Styrene Acrylonitrile Information provided by Polykemi AB |
|||
Flexural Modulus | 3.70 GPa | 537 ksi | ASTM D790 |
Solvay Specialty Polymers AvaSpire® AV-722 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-722 is an unreinforced polyaryletherketone (PAEK) that offers improved economics relative to PEEK while retaining most of PEEK's key performance attributes. AV-722 resin has been formula.. |
|||
Flexural Modulus | 3.70 GPa @Temperature 23.0 °C |
537 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYfill PP HIP8040F VT2 Polypropylene, Mineral Reinforced, Heat Resistant Information provided by Polykemi AB |
|||
Flexural Modulus | 3.70 GPa | 537 ksi | ISO 178 |
Nilit RECONYL A KV30 Recycled nylon 6.6 for injection molding, 30% glass ball reinforced Recycled nylon 6.6 for injection molding (available only in black).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Modulus | 3.70 GPa | 537 ksi | 1.5 mm/min; ISO 178:2001 |
Global EPP PA 6C MOLY Cast Polyamide 6 + MoS2 Cast nylons are generally accepted as the primary engineering polymer, suitable for virtually any plain bearing application. By varying the conditions of polymerisation the mechanical properties of .. |
|||
Flexural Modulus | 3.70 GPa | 537 ksi | |
Haysite HTF Polyester, High Temp Flex HTF exhibits excellent flexibility and retention of electrical properties at elevated temperatures. For use in 220º C insulation systems in dry type transformers and where flexibility and high te.. |
|||
Flexural Modulus | 3.70 GPa | 537 ksi | ASTM D790 |
IRPC Polimaxx Polene 1111NX TA4 Polypropylene Compound CHARACTERISTICS: POLYPROPYLENE HOMOPOLYMER WITH 20% TALCUM REINFORCEDAPPLICATIONS: INJECTION MOLDING FOR AUTOPARTS, ELECTRICAL APPLIANCES |
|||
Flexural Modulus | 3.70 GPa | 537 ksi | d.a.m., 2 mm/min; ISO 178-A |
Lanxess Durethan® A 30 S FN31 000000 Nylon 66, Flame Retardant PA 66, non-reinforced, injection molding, halogen-free flame retardant, improved flowabilityInformation provided by LANXESS. |
|||
Flexural Modulus | 3.70 GPa | 537 ksi | ISO 178 |
Solvay TECHNYL® B 738 MX15 Grey 3279 PA66/6, 15% mineral filled Description: TECHNYL B 738 MX15 Grey 3279 is a Polyamide 6.6, with 15% of mineral filler. Colors: GreyAvailable in: Latin AmericaMain Properties: ? Good Mechanical Properties, Good Superficial Aspec.. |
|||
Flexural Modulus | 3.70 GPa | 537 ksi | ASTM D790 |
Solvay Specialty Polymers KetaSpire® KT-850 Polyetheretherketone (PEEK) KetaSpire® KT-850 is the intermediate-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color pellet form. KetaSpire® PEEK is produced to the highest industry standa.. |
|||
Flexural Modulus | 3.70 GPa | 537 ksi | ISO 178 |
Solvay Specialty Polymers KetaSpire® KT-XXXX Polyetheretherketone (PEEK) KetaSpire® KT-820 is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a lubricated pellet form. KetaSpire® PEEK is produced to the highest industry standards and is cha.. |
|||
Flexural Modulus | 3.70 GPa | 537 ksi | ASTM D790 |
Solvay Specialty Polymers KetaSpire® KT-XXXX Polyetheretherketone (PEEK) KetaSpire® KT-820 is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a lubricated pellet form. KetaSpire® PEEK is produced to the highest industry standards and is cha.. |
|||
Flexural Modulus | 3.70 GPa | 537 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DFD029 PC (Europe-Africa-Middle East) LNP* Stat-kon* DFD029 is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant, Carbon Powder. Added features of this material include: Electrically Conductive, Flame Reta.. |
|||
Flexural Modulus | 3.70 GPa | 537 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP DX05477 PC LNP THERMOCOMP* DX05477 is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release, Flame Retardant. |
|||
Flexural Modulus | 3.70 GPa | 537 ksi | 3 points and 2 mm/min; ISO 178 |
Styron Pulse® 979 PC/ABS PULSE™ 979 is a high performance, 10% glass filled PC/ABS resin.Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Flexural Modulus | 3.70 GPa | 537 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Noryl GTX GTX977 PPE+PA66 (Asia Pacific) Noryl GTX GTX977 resin is a mineral reinforced conductive Noryl GTX with a improved CTE (7) with a balanced performance of Impact and stiffness. (developmental grade : EXNX0074)This data was supplie.. |
|||
Flexural Modulus | 3.70 GPa | 537 ksi | Tangent |
Schmelzer Industries Pearlveil 110-10 Fiberglass Veil Economical alternative for flat or shallow applications. Suitable for hand lay-up, pre-form molding, press molding, vacuum molding, and injection molding. Data provided by the manufacturer, Schmel.. |
|||
Flexural Modulus | 3.70 GPa | 537 ksi | ASTM D790 |
Unitika M1030B PA6, Dry Nano composite nylonInformation provided by Unitika Ltd. |
|||
Flexural Modulus | 3.70 GPa | 537 ksi | ASTM-D790 |
Polyram PlusTek RA325J5 Nylon 6.6, 25% Glass beads and Glass Fiber, Flame Retardant 25% glass beads and glass fiber reinforced, flame retardant polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Flexural Modulus | 3.70 GPa | 537 ksi | ISO 178-93 |
Wellman EcoLon® MRGF1619-WBK1 Mineral and Glass Reinforced Recycled Nylon 66 Description: Post Consumer Nylon Compound; WeatherableInformation provided by Wellman. |
|||
Flexural Modulus | 3.70 GPa | 537 ksi | ASTM-D790 |
Polyram RamTough PZ307G2 Polycarbonate, 10% Glass Fiber 10% glass fiber reinforced, UV stabilized polycarbonate for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Flexural Modulus | 3.70 GPa | 537 ksi | ASTM D 790 |
Cossa Polimeri ESTASAN SAN 3000 Styrene Acrylonitrile High melt flow rate, good chemical resistance, excellent dimensional stabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Flexural Modulus | 3.70 GPa | 537 ksi | DIN 52457 |
CP-Polymer-Technik Wellamid® 6600 MR 209 HWCP 20% Mineral Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Flexural Modulus | 3.70 GPa | 537 ksi | ASTM D790 |
Chem Polymer Chemlon 109-18 G Nylon 66, 18% Glass Fiber Reinforced A highly toughened 18% glass fiber reinforced nylon 66 developed for applications requiring stiffness, creep resistance and impact resistance.Data provided by the manufacturer, Chem Polymer. |
|||
Flexural Modulus | 3.70 GPa | 537 ksi | ASTM D790 |
Ashley Polymers Ashlene® 64M Nylon 66 A reinforced modified, platable nylon with high impact and excellent dimensional stability.Data provided by the manufacturer |