Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.67 GPa | 533 ksi | Tangent; ASTM D790 |
Fiberfil® J-68/30/E Polypropylene Copolymer, 30% Glass Fiber Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Flexural Modulus | 3.68 GPa @Thickness 3.20 mm |
533 ksi @Thickness 0.126 in |
15mm/min; ASTM D790 |
LG Chemical 80HF SAN, High Transparency, Heat Resistance, Chemical Resistance Feature: Injection Molding, SAN, High Transparency, Heat Resistance, Chemical ResistanceApplication: Refrigerator Sleeves, MiscellaneousCAS No. 9003-54-7Information provided by LG Chemical |
|||
Flexural Modulus | 3.68 GPa @Thickness 3.20 mm |
533 ksi @Thickness 0.126 in |
15mm/min; ASTM D790 |
LG Chemical 80HFICELLHK SAN, High Transparency, Heat Resistance, Chemical Resistance Feature: Injection Molding, SAN, High Transparency, Heat Resistance, Chemical ResistanceApplication: Refrigerator Sleeves, MiscellaneousCAS No. 9003-54-7Information provided by LG Chemical |
|||
Flexural Modulus | 3.67 GPa | 533 ksi | Tangent; ASTM D790 |
Fiberfil® J-68/30/E/UV Polypropylene Copolymer, 30% Glass Fiber Reinforced, Chemically coupled, UV Stabilized Information provided by FIBERFIL Engineered Plastics |