Mechanical Properties Metric English Comments
Flexural Modulus 3.56 GPa
516 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Cycoloy® CM6210 PC+ABS
Cycoloy* resin CM6210 is a high-modulus flame retardant PC/ABS with non-brominated and non-chlorinated FR system. It can be used for extrusion & thermoforming applications and also for injection mol..
Flexural Modulus 3.56 GPa
516 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Cycoloy® CM6210 PC+ABS (Asia Pacific)
Cycoloy* resin CM6210 is a high-modulus flame retardant PC/ABS with non-brominated and non-chlorinated FR system. It can be used for extrusion & thermoforming applications and also for injection mol..
Flexural Modulus 3.56 GPa
516 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Cycoloy® CM6210 PC+ABS (Europe-Africa-Middle East)
Cycoloy* resin CM6210 is a high-modulus flame retardant PC/ABS with non-brominated and non-chlorinated FR system. It can be used for extrusion & thermoforming applications and also for injection mol..
Flexural Modulus 3.56 GPa
516 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP LUBRICOMP RBL36XXJ PA 66
LNP* LUBRICOMP* RBL36XXJ is a compound based on Nylon 66 containing 30% Glass Bead, 15% PTFE. Added features of this grade include: Low Extractable, Healthcare, Wear Resistant.
Flexural Modulus 3.56 GPa
516 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP LUBRICOMP RX85514 PA 66
LNP LUBRICOMP* RX85514 is a compound based on Nylon 66 resin containing Proprietary Filler(s). Added features of this material include: Internally Lubricated.
Flexural Modulus 3.56 GPa
516 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP LUBRICOMP RX88514 PA 66
LNP LUBRICOMP* RX85514 is a compound based on Nylon 66 resin containing Proprietary Filler(s). AddedLNP LUBRICOMP* RX85514 is a compound based on Nylon 66 resin containing Proprietary Filler(s). A..
Flexural Modulus 3.56 GPa
516 ksi
ISO 178
DSM Fibre Intermediates Nyrim® 2025 (Wollastocoat®), Dry
Nyrim is a Block Copolymer of Nylon 6 and an elastomer with exceptional properties in impact resistance, fatigue and abrasion resistance. Nyrim is processed via Reaction Injection Moulding (RIM) tec..