Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.52 GPa | 510 ksi | ASTM D790 |
Nylene® Norpex® AX20MR , 20% Mineral Reinforced Polyphenylene Ether Description: Norpex® AX20MR is a 20% mineral reinforced Polyphenylene Ether. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Res.. |
|||
Flexural Modulus | 3.52 GPa | 510 ksi | ASTM D790 |
Polymer Resources PPX/NY G10 PPO/Nylon 66 Alloy , 10% Glass Reinforced Polyphenylene Oxide/Nylon 66 Alloy , 10% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa.. |
|||
Flexural Modulus | 3.52 GPa | 510 ksi | ASTM D790 |
Techmer ES Electrafil® NY-7/EC NAT PA6 |
|||
Flexural Modulus | 3.52 GPa | 510 ksi | ASTM D790 |
Techmer ES HiFill® PEI BK Availability: North AmericaForms: PelletsAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 3.52 GPa | 510 ksi | ASTM D790 |
Techmer ES HiFill® PEI HF BK Availability: North AmericaForms: PelletsFeatures: High FlowAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 3.52 GPa | 510 ksi | ASTM D790 |
Techmer ES HiFill® PEI TX5 LE Availability: North AmericaForms: PelletsAdditive: PTFE LubricantFeatures: Low Extractables and LubricatedInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 3.52 GPa | 510 ksi | ASTM D790 |
Techmer ES Luriblend® PA6/6 AF10 HS L Nylon 66 Availability: North AmericaForms: PelletsFiller/Reinforcement: Aramid Fiber, 10% Filler by WeightAdditive: Heat Stabilizer and PTFE Lubricant(10%)Features: Lubricated, Good Wear Resistance, Low Fric.. |
|||
Flexural Modulus | 3.52 GPa | 510 ksi | ASTM D790 |
Techmer ES Luriblend® PA6/6 AF10 Nylon 66 Availability: North AmericaForms: PelletsFiller/Reinforcement: Aramid Fiber, 10% Filler by WeightAdditive: LubricantFeatures: Lubricated, Good Wear Resistance and Low FrictionInformation provided by.. |
|||
Flexural Modulus | 3.52 GPa | 510 ksi | ASTM D790 |
Techmer ES Luriblend® PA6/6 GF10 M/TL10 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 10% Filler by WeightAdditive: Molybdenum Disulfide Lubricant and PTFE LubricantFeatures: LubricatedAppearance: Natural Col.. |
|||
Flexural Modulus | 3.52 GPa | 510 ksi | ASTM D790 |
Techmer ES Plaslube® J-1/AF/10/TF/10/HS BL8816 PA66 |
|||
Flexural Modulus | 3.52 GPa | 510 ksi | ASTM D790 |
Techmer ES Plaslube® J-1/AF/15/TF/10 NAT PA66 |
|||
Flexural Modulus | 3.52 GPa | 510 ksi | ASTM D790 |
Techmer ES Statiblend® PBT 03003 Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass FiberFeatures: Conductive, Antistatic and ESD ProtectionInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 3.52 GPa | 510 ksi | ASTM D790 |
Techmer ES Statiblend® PBT GF10 SS5 MB Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 10% Filler by WeightAdditive: AntistaticFeatures: Conductive, Antistatic and ESD ProtectionInformation provided by TP Comp.. |
|||
Flexural Modulus | 3.52 GPa | 510 ksi | ASTM D790 |
PlastxWorld CEVIAN® CGF20 20% GF PC/Acrylic Alloy Glass fiber reinforced PC/Acrylic alloy.These are typical values and are not intended for specification purposes. Information provided by PlastxWorld Inc. |
|||
Flexural Modulus | 3.52 GPa | 510 ksi | ASTM D790 |
Chase Plastics CP Pryme® PC110R Polycarbonate, 10% Glass Fiber Reinforced Features: Good mold releaseForm: PelletsInformation provided by Chase Plastics. |
|||
Flexural Modulus | 3.52 GPa | 510 ksi | Tangent; ASTM D790 |
Plastics Group Polifil® GFPPCC-20 20% Glass Reinforced Polypropylene Polifil® GFPPCC series compounds are homopolymer polypropylenes reinforced with chemically coupled glass fibers. These compounds offer superior strength and stiffness, improved elevated temperature.. |
|||
Flexural Modulus | 3.52 GPa | 510 ksi | ASTM D790 |
Chesterton ARC 10 Paste grade machinable composite Description: A reinforced composite for the repair and protection of metal surfaces. It is machinable with excellent compressive strength, chemical resistance and corrosion resistance. It is non-sag.. |
|||
Flexural Modulus | 3.52 GPa | 510 ksi | ASTM D790 |
Ensinger Tecatron® XP-78 Compression Molded PPS Compound, 47% PTFE Filled Seal Material Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p.. |
|||
Flexural Modulus | 3.52 GPa | 510 ksi | |
Abatron AboCast 8502-5/AboCure 8502-5 Colorless, Low-Exotherm Epoxy Casting Compound AboCast 8502-5/AboCure 8502-5 is a rigid, colorless, low-exotherm epoxy casting compound for spherical masses up to 500 grams. It is a 2-component structural and dielectric liquid system with extrem.. |
|||
Flexural Modulus | 3.52 GPa | 510 ksi | ASTM D790 |
Asahi Kasei Thermylene® P6-20FG-0753 20% Glass Fiber Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Flexural Modulus | 3.52 GPa | 510 ksi | ASTM D790 |
Polymer Resources PPX/NY G10 Modified PPO, 10% Glass Reinforced PPX/Nylon 6,6 Alloy
(Unverified Data**)&l Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Flexural Modulus | 3.52 GPa | 510 ksi | ASTM D790 |
Chesterton MRS 10 Metal Rebuilding System Description: A reinforced composite for the repair and protection of metal surfaces. It is machinable with excellent compressive strength, chemical resistance It is non-sagging, non-shrinking and 10.. |
|||
Flexural Modulus | 3.52 GPa | 510 ksi | ASTM D790 |
Techmer ES HiFill FR® PPO/HIPS MM20 FR 20% Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 20% Filler by Weight Features: Flame RetardantInformation provided by TP Composites, Inc. |