Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 34.5 GPa | 5000 ksi | ASTM D790 |
Quantum Composites QC-8816 66% Glass Fiber Reinforced Polyester Hybrid SMC QC-8816 is a polyester hybrid engineered structural composite molding compound reinforced with continuous, unidirectional (0°) glass fibers. It provides high strength, stiffness and fatigue resist.. |
|||
Flexural Modulus | 34.5 GPa | 5000 ksi | ASTM D790 |
Quantum Composites Lytex® 4149 55% Carbon Fiber Epoxy SMC Lytex 4149 is a high-performance, 3K tow carbon fiber (PAN) reinforced epoxy sheet molding compound designed for military and aerospace structural applications requiring excellent mechanical propert.. |
|||
Flexural Modulus | 34.5 GPa | 5000 ksi | Tangent; ASTM D790 |
Applied Composites 8068 Polyester SMC Industry Application: High StrengthProduct Application: MilitaryDistinct Features: Structural Grade Chopped and Unidirectional Fibers, High Stiffness, High Fiber LoadingsInformation provided by Appl.. |