Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.275 GPa | 475.0 ksi | ASTM D790 |
LG Chemical EG920 PMMA, General Purpose Grade for Extrusion General purpose grade with excellent stress cracking resistanceIntended mainly for exterior applicationsRecommended mainly for sheets, pipes, and profilesFeatures: Excellent transparency and eleganc.. |
|||
Flexural Modulus | 3.275 GPa | 475.0 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 234 20% Mineral Reinforced Ionomer / Nylon Alloy DescriptionFormion® FI 234 is an injection molding grade, 20% mineral reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance, high stiffness and lo.. |
|||
Flexural Modulus | 3.275 GPa | 475.0 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 234 20% Mineral Reinforced Ionomer / Nylon Alloy DescriptionFormion® FI 234 is an injection molding grade, 20% mineral reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance, high stiffness and lo.. |
|||
Flexural Modulus | 3.275 GPa | 475.0 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 234 20% Mineral Reinforced Ionomer / Nylon Alloy DescriptionFormion® FI 234 is an injection molding grade, 20% mineral reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance, high stiffness and lo.. |
|||
Flexural Modulus | 3.275 GPa | 475.0 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 234 20% Mineral Reinforced Ionomer / Nylon Alloy DescriptionFormion® FI 234 is an injection molding grade, 20% mineral reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance, high stiffness and lo.. |
|||
Flexural Modulus | 3.275 GPa | 475.0 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 234 20% Mineral Reinforced Ionomer / Nylon Alloy DescriptionFormion® FI 234 is an injection molding grade, 20% mineral reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance, high stiffness and lo.. |
|||
Flexural Modulus | 3.275 GPa | 475.0 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 234 20% Mineral Reinforced Ionomer / Nylon Alloy DescriptionFormion® FI 234 is an injection molding grade, 20% mineral reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance, high stiffness and lo.. |
|||
Flexural Modulus | 3.275 GPa | 475.0 ksi | ASTM Value |
BASF Capron® 8203C HS Blend Nylon 6 (Dry)
(discontinued **) Capron 8203C HS Blend is a heat stabilized, high viscosity nylon 6 extrusion compound possessing a modified crystalline structure for increased strength, stiffness and heat distortion temperature. .. |