Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.25 GPa | 471 ksi | |
Plastcom SLOVASTER® B1 GF 6 HML PBT, 6% glass fibre FeaturesPBT for injection moulding, chemically reinforced with 6 % glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending.. |
|||
Flexural Modulus | 3.25 GPa | 471 ksi | ASTM D790 |
Nylene® PA6/6 Homopolymer 134 HSL Nylon 6/6 Low Viscosity Nucleated Grade; Property data for dry as molded samples.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation. |
|||
Flexural Modulus | 3.25 GPa | 471 ksi | |
Plastcom SLOVASTER® B1 GF 6 PBT, 6% glass fibre FeaturesPBT for injection moulding, chemically reinforced with 6 % glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending.. |
|||
Flexural Modulus | 3.25 GPa @Temperature 90.0 °C |
471 ksi @Temperature 194 °F |
ISO 178, ASTM D790 |
Nilit Nilamid B G6 FR HF 30% Glass Fiber Reinforced, Flame Retardant PA6 Description: Nilamid B G6 FR HF is a NYLON 6 based flame retardant compound that does not contain any halogen or red phosphorous. It has a good overall mechanical performance, has an excellent price.. |
|||
Flexural Modulus | 3.25 GPa | 471 ksi | ASTM D790 |
I. Stern N2560 General Purpose Crystal Polystyrene Features:Excellent ClarityExcellent Process PropertiesHigh Heat MoldingApplicationsMedical PartsDomestic AppliancesAgency RatingsFDA Title 21 CFR 177.1640UL File E220962Information provided by I. St.. |
|||
Flexural Modulus | 3.25 GPa | 471 ksi | 2 mm/min; ISO 178 |
Inno-Comp INNOPOL® CS 1-1240 42% Chalk-Filled Polypropylene Homopolymer INNOPOL® CS 1-1240 is a 42% chalk –filled polypropylene homopolymer compound /PP-H KD42 (ISO 1043)/. This grade is available in natural and custom colored form.INNOPOL® CS 1-1240 is devel.. |
|||
Flexural Modulus | 3.25 GPa | 471 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP RAP22 PA 66 LNP* LUBRICOMP* RAP22 is a compound based on Nylon 66 resin containing 10% Aramid, 10% PTFE/Silicone. Added feature of this grade includes: Wear Resistant. |
|||
Flexural Modulus | 3.25 GPa | 471 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics ULTEM 1285 PEI (Europe-Africa-Middle East) Transparent Polyetherimide blend. ECO Conforming. US FDA and EU Food Contact compliant in recognized colors. |
|||
Flexural Modulus | 3.25 GPa | 471 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON KD000 Acetal Copolymer (Asia Pacific) LNP STAT-KON KD000* is also know as: LNP STAT-KON K, LNP STAT-KON KXC. It is a compound based on Acetal resin containing Carbon Powder. Added features of this material include: Electrically Conduct.. |
|||
Flexural Modulus | 3.25 GPa | 471 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON KD000 Acetal Copolymer (Europe-Africa-Middle East) LNP STAT-KON KD000* is also know as: LNP STAT-KON K, LNP STAT-KON KXC. It is a compound based on Acetal resin containing Carbon Powder. Added features of this material include: Electrically Conduct.. |
|||
Flexural Modulus | 3.25 GPa | 471 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON KD000 Acetal Copolymer LNP* STAT-KON* KD000 is a compound based on Acetal resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |
|||
Flexural Modulus | 3.25 GPa | 471 ksi | 2mm/min; ISO 178 |
Borealis MG302Al Polypropylene Compound, Mineral Filled MG302AI is a 30% mineral filled polypropylene compound intended for injection and back injection molding. This material has an excellent balance between impact strength and stiffness and high melt .. |
|||
Flexural Modulus | 3.25 GPa @Temperature 93.0 °C |
471 ksi @Temperature 199 °F |
ASTM Test |
BASF Ultramid® 8333G HI 33% Glass Filled PA6 (Conditioned) Ultramid 8333G HI is a 14% glass reinforced, impact modified PA6 injection molding compound developed for applications requiring improved dry as molded toughness in combination with a
balance of st.. |
|||
Flexural Modulus | 3.25 GPa | 471 ksi | ISO 178 |
Ascend Performance Materials Vydyne® R515 Nylon 66, 15% Glass Reinforced, Conditioned Vydyne® R515 is general-purpose, 15% glass-fiber reinforced PA66 resin. Availability:Asia PacificEuropeNorth AmericaFiller/Reinforcement:Glass Fiber, 15% Filler by WeightAdditive:Lubricant Features.. |
|||
Flexural Modulus | 3.25 GPa | 471 ksi | ISO 178 |
Ineos Nova 201 Crystal Polystyrene High Heat Extrusion Grade
(discontinued **) Excellent heat resistance, Superior melt strengthApplications: Foam insulation, Oriented polystyrene sheet (OPS), XPS food packaging, Sheet and profile extrusionProperties were determined on injecti.. |
|||
Flexural Modulus | 3.25 GPa | 471 ksi | ISO 178 |
Ascend Performance Materials Vydyne® R515H Nylon 66, 15% Glass Reinforced, Conditioned Vydyne® R515H is general-purpose, heat-stabilized, hydrolysis-resistant, 15% glass-fiber reinforced PA66 resin. Available in natural it is specifically designed to maximize the retention of physica.. |