Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.169 GPa | 459.6 ksi | tangent; chs 0.05 in/min; ASTM D790 |
Diamond Polymers GPPS BEADS Injection Molding Grade, General Purpose Polystyrene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Flexural Modulus | 3.169 GPa | 459.6 ksi | tangent; chs 0.05 in/min; ASTM D790 |
Diamond Polymers NPS80-1800B Injection Molding Grade, General Purpose Polystyrene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Flexural Modulus | 3.169 - 3.238 GPa | 459.6 - 469.6 ksi | 90 Minute UV Cure; ASTM D790 |
3D Systems Accura® SI 40 Plastic for the SLA® 250 System Accura 40 "Ar" or "Hc" type materials - for the SLA 250 system. Mimics Nylon 6:6ApplicationsHigh temperature testing:Under hood bolt-on testingWind tunnel testingHVAC testingPrototyping and testing .. |