Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.931 GPa | 425.1 ksi | ASTM D790 |
Lucent Polymers GPP-220 Polypropylene, 20% Glass Fiber Reinforced, Chemically Coupled, Impact Modified Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |