Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.81 GPa | 408 ksi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Extrusion L0152 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Flexural Modulus | 2.81 GPa | 408 ksi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Extrusion LR610 white 1046 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Modulus | 2.81 GPa | 408 ksi | Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790 |
Network Polymers MS 125 Styrene Methyl Methacrylate Terpolymer Description: Styrene Methyl Methacrylate TerpolymerInformation provided by Network Polymers Inc. |
|||
Flexural Modulus | 2.81 GPa | 408 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycolac® MG37EPX ABS ABS plating grade optimized for a broad processing window for both painted and plated applications. NSF standard 61 compliant (80 sq in/L) |
|||
Flexural Modulus | 2.81 GPa | 408 ksi | ASTM D790 |
Nilit Polynil® P230 High Viscosity Nylon 66 Description: Polynil P230 is a high viscosity NYLON 66 (Viscosity number 280 cm³/gr) that was developed for film- and rod extrusion. It has high melt stability and low gel content. It holds various.. |
|||
Flexural Modulus | 2.81 GPa | 408 ksi | ASTM D790 |
Nilit Polynil® P240 High Viscosity Nylon 66 Description: Polynil P240 is a high viscosity NYLON 66 (Viscosity number 290 cm³/gr) that was developed for rod and slab extrusion. It has a high melt stability and a low gel content.Key characteri.. |
|||
Flexural Modulus | 2.81 GPa | 408 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycoloy® CX7720 PC+ABS (Asia Pacific) Cycoloy resin CX7720 is a non brominated and non chlorinated flame retardant PC/ABS resin grade featuring high heat resistance and thin wall FR. It is UL-94 listed at 1.2 mm V0 and 1.5mm 5VB. Its hi.. |
|||
Flexural Modulus | 2.81 GPa | 408 ksi | ASTM D790 |
PolyOne Edgetek® NN-35MG/000 Black v1.1 Polyamide 66 (Nylon 66) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Flexural Modulus | 2.81 GPa | 408 ksi | ASTM D790 |
PolyOne Geon™ Vinyl Dry Blend E6755 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Modulus | 2.81 GPa | 408 ksi | ASTM D790 |
SABIC Innovative Plastics LNP FARADEX AS002 ABS LNP* Faradex* AS002 is a compound based on Acrylonitrile Butadiene Styrene resin containing 10% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding... |
|||
Flexural Modulus | 2.81 GPa | 408 ksi | ASTM D790 |
SABIC Innovative Plastics LNP FARADEX AS002 ABS (Asia Pacific) LNP* Faradex* AS002 is a compound based on Acrylonitrile Butadiene Styrene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Flexural Modulus | 2.81 GPa | 408 ksi | ASTM D790 |
SABIC Innovative Plastics LNP FARADEX AS002 ABS (Europe-Africa-Middle East) LNP* Faradex* AS002 is a compound based on Acrylonitrile Butadiene Styrene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Flexural Modulus | 2.81 GPa | 408 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP EL002 PEI LNP* Lubricomp* EL002 is a compound based on Polyetherimide resin containing 10% PTFE. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 2.81 GPa | 408 ksi | 2 mm/min, 64mm span; ISO 178 |
SABIC Innovative Plastics SABIC PPCOMPOUND 55T1030 PP SABIC® PPcompound 55T1030 is a general purpose, talc filled, heat stabilized copolymer polypropylene compound. This compound exhibits very high impact, and is suitable for multiple processing met.. |
|||
Flexural Modulus | 2.81 GPa | 408 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DX00887C PC LNP STAT-KON* DX00887C is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Clean Compounding System, Electrically Conductive. |
|||
Flexural Modulus | 2.81 GPa | 408 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP DX09402 PC LNP* THERMOCOMP* DX09402 is a compound based on Polycarbonate containing Proprietary Filler(s). |
|||
Flexural Modulus | 2.81 GPa | 408 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOTUF MX00619 PP LNP* Thermotuf* MX00619 is a compound based on Polypropylene resin containing Proprietary Filler(s). |
|||
Flexural Modulus | 2.81 GPa | 408 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOTUF MX00619 PP (Asia Pacific) LNP* Thermotuf* MX00619 is a compound based on Polypropylene resin containing Proprietary Filler(s). |