Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.0296 GPa | 4.30 ksi | 1% secant; ASTM D790 |
ExxonMobil Escorene® UL 7765 Adhesive Application Resin Escorene Ultra UL 7765 is a high viscosity, 26.2% vinyl acetate copolymer that has very good flexibility and low temperature toughness. It has good compatibility with both hydrocarbon and natural t.. |
|||
Flexural Modulus | 0.0296 GPa | 4.30 ksi | 2% Secant; Molded and tested in accordance with ASTM D4976; ASTM D790 A |
Dow FLEXOMER™ DFDA-1095 NT Very Low Density Polyethylene (VLDPE) Resin FLEXOMER™ DFDA-1095 NT is an ethylene-butene copolymer with a unique olefinic composition for improved process-ability and material handling. This product is produced via gas phase polymerization .. |