Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.75 GPa @Thickness 3.20 mm |
398 ksi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical HI121H ABS, High Stiffness Feature: Injection Molding, High StiffnessApplication: Electric & Electronic Products, Miscellaneous GoodsCAS No. 9003-56-9Information provided by LG Chemical |
|||
Flexural Modulus | 2.75 GPa @Thickness 3.20 mm |
398 ksi @Thickness 0.126 in |
15mm/min; ASTM D790 |
LG Chemical LUCON CP6062EX PC/ABS+CNT Description: Sheet Extrusion or Injection Molding, PC/ABS+CNT, Electrostatic Dissipation, Wide Processing Range, Low Surface ResistivityApplication: BLU Carrying TrayCAS No. 103598-77-2, 9003-56-9, .. |
|||
Flexural Modulus | 2.75 GPa | 398 ksi | DIN 53452; ASTM D790 |
Kolon KOPA® KN111 General Purpose Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Flexural Modulus | 2.75 GPa @Thickness 3.20 mm |
398 ksi @Thickness 0.126 in |
2.8mm/min; ASTM D790 |
LG Chemical LUMID GP1000B(W) PA66, General Purpose, Low Viscosity Feature: Injection Molding, PA66, General Purpose, Low ViscosityApplication: Buckles, Chair NobCAS No. 32131-17-2Information provided by LG Chemical |
|||
Flexural Modulus | 2.75 GPa @Thickness 3.20 mm |
398 ksi @Thickness 0.126 in |
15mm/min; ASTM D790 |
LG Chemical LUMIPLAS LD590 Light diffusion ABS Description: Injection Molding, Light diffusion, Medium ImpactApplication: (LED) Lamp Cover, Signboard Lighting Decoration of Electronic DeviceCAS No. 9010-94-0Information provided by LG Chemical |
|||
Flexural Modulus | 2.75 GPa @Thickness 6.40 mm |
398 ksi @Thickness 0.252 in |
1.3mm/min; ASTM D790 |
LG Chemical LUPOL GP2150 PP+GF15% Description: Injection Molding, PP+GF15%, General PurposeApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 65997-17-3Information provided by LG Chemical |
|||
Flexural Modulus | 2.75 GPa @Thickness 6.40 mm |
398 ksi @Thickness 0.252 in |
30mm/min; ASTM D790 |
LG Chemical LUPOL GP3200 PP+MF20% Description: Injection Molding, PP+MF10%, General PurposeApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical |
|||
Flexural Modulus | 2.75 GPa | 398 ksi | DIN 53452; ASTM D790 |
Kolon KOPA® KN333HRN Heat Resistant Nylon 66 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin.. |
|||
Flexural Modulus | 2.75 GPa @Thickness 3.20 mm |
398 ksi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY GN5001RFP PC/ABS, Halogen Free Flame Retardant, Heat Resistance Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, General PurposeApplication: E&E (TV, Navigation Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Ch.. |
|||
Flexural Modulus | 2.75 GPa @Thickness 3.20 mm |
398 ksi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical PI642G ABS, General Purpose, High Modulus Feature: Extrusion Molding, General Purpose, High ModulusApplication: Pipe fittingCAS No. 9003-56-9Information provided by LG Chemical |
|||
Flexural Modulus | 2.75 GPa | 398 ksi | DIN 53452; ASTM D790 |
Kolon KOPA® KN133HR Heat Resistant Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Flexural Modulus | 2.75 GPa @Thickness 6.40 mm |
398 ksi @Thickness 0.252 in |
30mm/min; ASTM D790 |
LG Chemical LUPOL HR2100D PP+GF17% Description: Injection Molding, PP+GF17%, General PurposeApplication: Electrical, Electronic and Automotive Parts CAS: 9003-07-0 and 165997-17-3Information provided by LG Chemical |
|||
Flexural Modulus | 2.75 GPa @Thickness 3.20 mm |
398 ksi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical XG568 MABS, Anti-Scratch, High Gloss Feature: Injection Molding, Anti-Scratch, High GlossApplication: LCD TV Front Cabinet, Bezel, Audio/Video HousingCSA No. 9011-14-7 and 9003-56-9Information provided by LG Chemical |
|||
Flexural Modulus | 2.75 GPa | 398 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® NE-1010 PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.75 GPa | 398 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® NE-1010 PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.74 GPa | 398 ksi | ASTM D790 |
A. Schulman ComAlloy® E-14756 Flame Retardant Easy Flow Polycarbonate Alloy Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 2.74 GPa | 398 ksi | ASTM D790 |
A. Schulman ComAlloy® E-14756 Flame Retardant Easy Flow Polycarbonate Alloy Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 2.74 GPa | 398 ksi | ASTM D790 |
A. Schulman ComAlloy® E-14756 Flame Retardant Easy Flow Polycarbonate Alloy Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 2.74 GPa | 398 ksi | ASTM D790 |
A. Schulman ComAlloy® E-14756 Flame Retardant Easy Flow Polycarbonate Alloy Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 2.74 GPa | 398 ksi | ASTM D790 |
A. Schulman ComAlloy® E-14756 Flame Retardant Easy Flow Polycarbonate Alloy Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 2.74 GPa | 398 ksi | ASTM D790 |
A. Schulman ComAlloy® E-14756 Flame Retardant Easy Flow Polycarbonate Alloy Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 2.75 GPa @Thickness 6.40 mm |
398 ksi @Thickness 0.252 in |
5 mm/min; ASTM D790 |
Bhansali Engineering Abstron IM14GL ABS Injection Molding Grade Super High Rigidity, Medium Impact, High Chemical ResistanceInformation provided by Bhansali |
|||
Flexural Modulus | 2.75 GPa | 398 ksi | 2.8mm/min; ASTM D790 |
Asia International Enterprise (Hong Kong) 3010F Polybutylene terephthalate Information provided by Asia International Enterprise (Hong Kong) Ltd. |
|||
Flexural Modulus | 2.74 GPa | 398 ksi | ASTM D790 |
Aaron Industries AAROPRENE® AEN 6000-1 Nylon 6 Engineered Resin |
|||
Flexural Modulus | 2.75 GPa @Thickness 3.20 mm |
398 ksi @Thickness 0.126 in |
ASTM D790 |
Supreme Petrochem SP 6605 Toughened Polystyrene Characteristics Excellent melt strength High stiffness Easy tearability Processing Extrusion Applications Suitable for thin film for candy wrap and window envelope Economic production of clear th.. |
|||
Flexural Modulus | 2.74 GPa | 398 ksi | ASTM D790 |
Quadrant EPP Quadrant PVC Polyvinyl Chloride, Type I, Grade 1 (ASTM Product Data Sheet) |
|||
Flexural Modulus | 2.75 GPa @Thickness 6.40 mm |
398 ksi @Thickness 0.252 in |
5 mm/min; ASTM D790 |
Bhansali Engineering Abstron IM14GL ABS Injection Molding Grade Super High Rigidity, Medium Impact, High Chemical ResistanceInformation provided by Bhansali |