Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.69 GPa | 390 ksi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Molding MR201 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Modulus | 2.69 GPa | 390 ksi | ASTM D790 |
NYCOA 400 PA 6 nucleated general molding gradeInformation provided by NYCOA, Inc. |
|||
Flexural Modulus | 2.69 GPa | 390 ksi | ASTM D790 |
Polymer Resources PC/ABS-FRG5 Flame Retardant PC/ABS Alloy, 5% Glass Reinforced PC/ABS Alloy, Flame Retardant, 5% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr.. |
|||
Flexural Modulus | 2.69 GPa @Thickness 3.17 mm |
390 ksi @Thickness 0.125 in |
ASTM D790 |
PTS PCA-2201NH Non Bromine, Non Chlorine Flame Retardant Polycarbonate/ABS Alloy Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Modulus | 2.69 GPa @Thickness 3.17 mm |
390 ksi @Thickness 0.125 in |
ASTM D790 |
PTS PCA-2201NHV Non Bromine, Non Chlorine Flame Retardant Polycarbonate/ABS Alloy, UV Stabilized Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Modulus | 2.69 GPa | 390 ksi | ASTM D790 |
Omni Plastics OmniTech™ HPP TF20 V0 Flame Retardant OmniTech™ is a family of non-standard products custom developed for applications with unique functional requirements, including but not limited to: Flame Retardant, Conductive, Wear Resistant, and .. |
|||
Flexural Modulus | 2.69 GPa | 390 ksi | ASTM D790 |
Polymer Resources PC/ABS-FR1-[color]-HH Flame Retardant PC/ABS Alloy, Low Flow PC/ABS Alloy, Flame Retardant, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by P.. |
|||
Flexural Modulus | 2.69 GPa | 390 ksi | ASTM D790 |
PolyOne Lubri-Tech™ AS-10GB/02S Acrylonitrile Butadiene Styrene (ABS), Glass Bead Filled
(discontinued **)< Description/Features:Glass Bead FilledSilicone LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 2.69 GPa | 390 ksi | ASTM D790 |
Solvay Specialty Polymers Udel® P-1710 Polysulfone (PSU)
(Unverified Data**) Udel P-1710 polysulfone (PSU) is a tough, rigid, high-strength thermoplastic that is suitable for continuous use up to 300°F (149°C). The resin is resistant to oxidation and hydrolysis and withsta.. |
|||
Flexural Modulus | 2.69 GPa | 390 ksi | ASTM D790 |
Solvay Specialty Polymers Udel® P-1720 Polysulfone (PSU)
(discontinued **) Udel P-1720 is a flame-retardant grade of polysulfone (PSU) that has a UL94 rating of V-0 at a thickness of 1 mm (0.039"). In general, polysulfone is a tough, rigid, high-strength thermoplastic that.. |
|||
Flexural Modulus | 2.69 GPa | 390 ksi | ASTM D790 |
Solvay Specialty Polymers Udel® P-1750 MR Polysulfone (PSU)
(Unverified Data**) Udel P-1750 MR is a lower color grade of polysulfone that contains a mold release which aids part ejection when parts with low draft are injection molded. Polysulfones have long been known for trans.. |
|||
Flexural Modulus | 2.69 GPa | 390 ksi | ASTM D790 |
Solvay Specialty Polymers Udel® P-3500 LCD Polysulfone (PSU)
(Unverified Data**) Udel P-3500 LCD is a very high molecular weight grade of polysulfone, and therefore offers the greatest toughness and chemical resistance of the available grades. It is well-suited for extrusion. Th.. |
|||
Flexural Modulus | 2.69 GPa | 390 ksi | ASTM D790 |
Solvay Specialty Polymers Udel® P-3703 Polysulfone (PSU)
(Unverified Data**) Udel P-3703 is a high-flow grade of polysulfone intended for injection molding applications with thin walls or long flow lengths. This grade has higher flow than Udel P-1700 and a slightly greater t.. |
|||
Flexural Modulus | 2.69 GPa | 390 ksi | ASTM D790 |
Solvay Specialty Polymers Udel® P-1835 Polysulfone (PSU)
(discontinued **) Udel P-1835 polysulfone is a powdered grade well suited for the fabrication of porous membranes. The membranes can be made into hollow fibers, tubes, plates, or spiral wound elements. They are used .. |
|||
Flexural Modulus | 2.69 GPa | 390 ksi | Molded; ASTM D790 |
Honeywell Aegisâ„¢ H135MP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H135MP is a lubricated and nucleated high viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR.. |
|||
Flexural Modulus | 2.69 GPa | 390 ksi | Tangent; ASTM D790 |
Fiberfil® J-60/10/E/M Polypropylene Homopolymer, 10% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Flexural Modulus | 2.69 GPa | 390 ksi | ASTM-D790 |
Ineos ABS Lustran® ABS 349 Lustran® ABS 349 is a high-gloss, medium-impact injection molding resin that has been specially formulated for excellent surface lubricity using internal additives. |
|||
Flexural Modulus | 2.69 GPa | 390 ksi | ASTM D790 |
Solvay Specialty Polymers Udel® P-3703 Polysulfone (PSU) Udel® P-3703 is a high-flow grade of polysulfone intended for injection molding applications with thin walls or long flow lengths. This grade has higher flow than Udel® P-1700 and a slightly g.. |
|||
Flexural Modulus | 2.69 GPa | 390 ksi | ASTM D790 |
Techmer ES HiFill® PBT HS BK Availability: North AmericaForms: PelletsAdditive: Heat StabilizerFeatures: Good Flow, Good Processability and Heat StabilizedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 2.69 GPa | 390 ksi | ASTM D790 |
Techmer ES Luriblend® POM CO TL10 Acetal Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant(10%)Features: Lubricated, Good Wear Resistance, Low Friction and CopolymerInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 2.69 GPa | 390 ksi | ASTM D790 |
Techmer ES Plastiblend® PC/ABS FR 1950 BK Availability: North AmericaForms: PelletsFeatures: Flame RetardantAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 2.69 GPa @Thickness 3.20 mm |
390 ksi @Thickness 0.126 in |
Injection Molded; ASTM D790 |
Styron EMERGEâ„¢ 7700 Polycarbonate (PC) / Acrylonitrile Butadiene Styrene (ABS) Overview: EMERGEâ„¢ PC/ABS 7700 Advanced Resin is an ignition-resistant PC/ABS blend that contains no chlorine for bromine additives. It has superior processability for injection molding applicat.. |
|||
Flexural Modulus | 2.69 GPa | 390 ksi | ASTM D790 |
Westlake Plastics Corzan® II CPVC Sheet Corzan® II CPVC, manufactured from Corzan G2 resin, was developed for use in the construction of wet benches and other cleanroom equipment for the semiconductor industry. It meets Factory Mutual.. |
|||
Flexural Modulus | 2.69 GPa @Temperature 22.8 °C |
390 ksi @Temperature 73.0 °F |
ASTM D790 |
Ensinger HYDEX® 4101L Polybutylene Terephthalate (PBT) HYDEX® 4101 & 4101L (lubricated) is a very stable chemical compound that can withstand high impact without deterioration. It is approved for direct contact with food by the FDA and is ideal for ma.. |
|||
Flexural Modulus | 2.69 GPa @Temperature 22.8 °C |
390 ksi @Temperature 73.0 °F |
ASTM D790 |
Ensinger TECASON™ S Polysulfone (PSU) TECASON™ S is a transparent engineering plastic known for its chemical resistance, rigidity, high-temperature performance, and its ability to operate in an autoclave environment. TECASON™ S is FD.. |
|||
Flexural Modulus | 2.69 GPa | 390 ksi | ASTM D790 |
Amco Amalloy® B1172 Polymer Alloy Amco Amalloy B1172 is a proprietary copolymer with exceptional clarity and enhanced impact strength.Impact modified, very clear, moderate flow.Information provided by Amco Plastic Materials. |
|||
Flexural Modulus | 2.69 GPa | 390 ksi | ASTM D790 |
Aaron Industries AVPS H 100-3 Virgin Polystyrene Melt flow index may be specified. |
|||
Flexural Modulus | 2.69 GPa | 390 ksi | |
Abatron AboCast 8103-13 One-Component Epoxy AboCast 8103-13 is the low-viscosity one-component clear epoxy system with deep impregnation that offers high performance at relatively high temperatures. It is best for thin-wall casting. Suggested.. |