Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.363 GPa | 342.7 ksi | ASTM D790 |
LG Chemical HI835M PMMA, Impact Resistant Grade Molding granule designed for greater impact strength combined with the outstanding properties of conventional acrylic materialsFeatures: Excellent transparency and eleganceWeather resistance and che.. |