Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 23.5 GPa | 3410 ksi | ASTM D790 |
PolyOne Stat-Tech™ X ST6600-0040 ES FR Black Polyamide 66 (Nylon 66) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Flexural Modulus | 23.5 GPa | 3410 ksi | ASTM D790 |
LNP Stat-Kon® OC-1006 Polyphenylene Sulfide, Carbon Fiber Reinforcement
(discontinued **) Features: Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades.. |
|||
Flexural Modulus | 23.5 GPa @Temperature 23.0 °C |
3410 ksi @Temperature 73.4 °F |
ISO 178 |
Victrex® PEEK 90GL60 Polyetheretherketone, 60% Glass Fibre Reinforced Product Description:High performance thermoplastic material, 60% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, standard flow, FDA food contac.. |
|||
Flexural Modulus | 23.5 GPa @Temperature 23.0 °C |
3410 ksi @Temperature 73.4 °F |
ISO 178 |
Victrex® PEEK -HT™ 22CA30 PolyEtherKetone, 30% Carbon Fibre Reinforced Product Description:High performance thermoplastic material, 30% carbon fibre reinforced PolyEtherKetone (PEK), semi crystalline, granules for injection moulding, standard flow, FDA food contact com.. |
|||
Flexural Modulus | 23.5 GPa @Temperature 23.0 °C |
3410 ksi @Temperature 73.4 °F |
ISO 178 |
Victrex® ST™ ST45CA30 PolyEtherKetoneEtherKetoneKetone, 30% Carbon Fibre Reinforced Product Description:High performance thermoplastic material, 30% carbon fibre reinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, granules for injection moulding, standard flow, .. |
|||
Flexural Modulus | 23.5 GPa | 3410 ksi | ISO 178 |
Solvay Specialty Polymers Ixef® 1032 Polyarylamide (PARA)
(Unverified Data**) Ixef 1032 is a 60% glass-fiber reinforced, general purpose polyarylamide compound which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance. - Natural.. |
|||
Flexural Modulus | 23.5 GPa | 3410 ksi | ISO 178 |
Solvay Specialty Polymers Ixef® 1032 Polyarylamide (PARA), 60% Glass Fiber (Dry) Ixef® 1032 is a 60% glass-fiber reinforced, general purpose polyarylamide compound which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Featur.. |
|||
Flexural Modulus | 23.5 GPa | 3410 ksi | GB/T 9341-2008 |
Sichuan Deyang Haton® hGC51 PPS / AE Polyphenylene Sulfide Injection molding, conductiveInformation provided by Sichuan Deyang Chemical Co., LTD |
|||
Flexural Modulus | 23.51 GPa | 3410 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON OE006A PPS - Branched LNP STAT-KON* OE006A is a compound based on PPS - Branched resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive. |