Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.345 GPa | 340.1 ksi | ASTM D790 |
Lucent Polymers PC-1403 Polycarbonate, Extrusion/Blow Molding Grade Medium FlowAdd "R" for Added ReleaseAdd "U" for UVÂ StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Flexural Modulus | 2.345 GPa | 340.1 ksi | ASTM D790 |
Lucent Polymers PC-1403FD Polycarbonate, FDA Compliant, Extrusion/Blow Molding Grade Medium FlowAdd "R" for Added ReleaseAdd "U" for UVÂ StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Flexural Modulus | 2.345 GPa | 340.1 ksi | ASTM D 790 |
MRC Polymers NAXALOYâ„¢ 773 ABS + PC Alloy Information provided by MRC Polymers Inc. |
|||
Flexural Modulus | 2.345 GPa | 340.1 ksi | tangent; chs 0.05 in/min; ASTM D790 |
Diamond Polymers ABS 3501 Natural 1002 ESCR Injection Molding Grade, Environmental Stress Crack Resistant Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Flexural Modulus | 2.345 GPa | 340.1 ksi | tangent; chs 0.05 in/min; ASTM D790 |
Diamond Polymers ABS 3501E Natural 1002 ESCR Extrusion Grade, Environmental Stress Crack Resistant Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Flexural Modulus | 2.345 GPa | 340.1 ksi | tangent; chs 0.05 in/min; ASTM D790 |
Diamond Polymers ABS 3501E-1300 Extrusion Grade, High Impact Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Flexural Modulus | 2.345 GPa | 340.1 ksi | ASTM D790 |
Ineos Nova 5100 High Impact Polystyrene
(discontinued **) Good balance of toughness and rigidity, USP Class VIApplications: Spools and reels, Thermoformed and molded packaging, Photographic cartridges, AppliancesProperties were determined on injection mold.. |
|||
Flexural Modulus | 2.345 GPa | 340.1 ksi | ASTM D790 |
Ineos Nova 5104 High Impact Polystyrene
(discontinued **) Good balance of toughness and rigidity, USP Class VIApplications: Spools and reels, Thermoformed and molded packaging, Photographic cartridges, AppliancesProperties were determined on injection mold.. |
|||
Flexural Modulus | 2.345 GPa | 340.1 ksi | ASTM D790 |
Lucent Polymers TPP-330 Polypropylene, 30% Talc Filled, Impact Modified Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |