Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.234 GPa | 34.0 ksi | 1% Secant; ASTM D790 |
Multibase Multi-Flex® D 3902 MRS TPE Thermoplastic Elastomer Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase |
|||
Flexural Modulus | 0.234 GPa | 34.0 ksi | ASTM D790 |
LyondellBasell Petrothene® NA940000 Low Density Polyethylene (Blow Molding) ApplicationsPETROTHENE NA 940-000 is a low density homopolymer resin intended for use in blow molding applications. Excellent toughness, good clarity and processability make NA 940-000 an ideal cho.. |
|||
Flexural Modulus | 0.234 GPa | 34.0 ksi | Molded; ASTM D790 |
LyondellBasell Petrothene® NA940085 Low Density Polyethylene (Film Grade) ApplicationsPETROTHENE NA 940 is a series of resins designed for heavy duty film applications. Superior puncture resistance combined with excellent impact properties make NA 940 an ideal choice for.. |
|||
Flexural Modulus | 0.234 GPa | 34.0 ksi | Molded; ASTM D790 |
LyondellBasell Petrothene® NA940094 Low Density Polyethylene (Film Grade) ApplicationsPETROTHENE NA 940 is a series of resins designed for heavy duty film applications. Superior puncture resistance combined with excellent impact properties make NA 940 an ideal choice for.. |
|||
Flexural Modulus | 0.234 GPa | 34.0 ksi | 2% Secant; Molded and tested in accordance with ASTM D4976; ASTM D790 B |
Dow 722 Linear Low Density Polyethylene (LDPE) DOW Polyethylene 722 is a broad molecular weight distribution homopolymer designed to offer good impact strength and rack resistance, with excellent flexibility. Typical applications include caps/c.. |
|||
Flexural Modulus | 0.234 GPa | 34.0 ksi | ASTM D790 |
Lubrizol ESTANE® 58142 Ester Based Thermoplastic Polyurethane Features: Fast cycling, broad temperature performance, and durabilityUse: Injection Molding Available in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol. |
|||
Flexural Modulus | 0.234 GPa | 34.0 ksi | Molded; ASTM D790 |
LyondellBasell Petrothene® NA940000 Low Density Polyethylene (Film Grade) ApplicationsPETROTHENE NA 940 is a series of resins designed for heavy duty film applications. Superior puncture resistance combined with excellent impact properties make NA 940 an ideal choice for.. |