Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.29 GPa | 332 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® FXD1433T PC Copolymer Clear PC-siloxane copolymer with excellent processability in special light diffusion colors. Medium flow, UV stabilized. Improved toughness compared to standard PC in same color. Color package may .. |
|||
Flexural Modulus | 2.29 GPa | 332 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® FXD1433T PC Copolymer (Asia Pacific) Clear PC-siloxane copolymer with excellent processability in special light diffusion colors. Medium flow, UV stabilized. Improved toughness compared to standard PC in same color. Color package may .. |
|||
Flexural Modulus | 2.29 GPa | 332 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® FXD1433T PC Copolymer (Europe-Africa-Middle East) Clear PC-siloxane copolymer with excellent processability in special light diffusion colors. Medium flow, UV stabilized. Improved toughness compared to standard PC in same color. Color package may .. |
|||
Flexural Modulus | 2.29 GPa | 332 ksi | ASTM D790 |
Albis Plastics PC/PET 361E Unfilled
(discontinued **) Amorphous Polycarbonate /Polyethylene Terephthalate Blend (PC/PET)Characteristics: High Strength, Rigidity and Creep Resistance. Good Chemical ResistanceApplications: Pump Components, Industrial and.. |
|||
Flexural Modulus | 2.29 GPa | 332 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP COLORCOMP DX06407H PC LNP* COLORCOMP* DX06407H is an unfilled Polycarbonate. Added features of this material include: Easy Molding, Mold Release, Healthcare |
|||
Flexural Modulus | 2.29 GPa | 332 ksi | (102 mm Span) 3mm/min; ASTM D790 |
LNP ULTEM® SMU5872 Polyetherimide, 25% PTFE Lubricant
(discontinued **) Not stand-alone resin: Compounding/ concentrate for wear resistance. Will be commercialized as UF2500.Features: Lubricated, Good Wear ResistanceForms: PelletsInformation provided by LNP, a GE Plasti.. |
|||
Flexural Modulus | 2.29 GPa | 332 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP DX09410H PC LNP* LUBRICOMP* DX09410H is a compound based on Polycarbonate resin containing Proprietary FIllers. Added features of this grade include: Healthcare, Wear Resistant. |
|||
Flexural Modulus | 2.29 GPa | 332 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP ZP001XXP PPE+PS LNP* LUBRICOMP* ZP001XXP is a compound based on PPE+PS resin containing 5% PTFE/Silicone. Added features of this material include: Wear Resistant. |
|||
Flexural Modulus | 2.29 GPa | 332 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® 175 PBT Unreinforced, neat PBT resin for compounding only. Natural Color Only, Not intended for injection molding.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 2.29 GPa | 332 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® 175 PBT (Europe-Africa-Middle East) Unreinforced, neat PBT resin for compounding only. Natural Color Only, Not intended for injection molding. |
|||
Flexural Modulus | 2.29 GPa | 332 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® 176 PBT Unreinforced, neat PBT resin for fibers. Natural Color Only, Not intended for injection molding. |
|||
Flexural Modulus | 2.29 GPa | 332 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® 176HP PBT Unreinforced, FDA compliant neat PBT resin for fibers. Natural Color Only, Not intended for injection molding. |
|||
Flexural Modulus | 2.29 GPa | 332 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Xenoy® X6125 PBT+PC Unreinforced, impact modified, thermoplastic alloy (PBT+PC). High impact strength while retaining mechanical and thermal properties.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 2.29 GPa | 332 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp DX93681 PC LNP* Thermocomp* DX93681 is a compound based on Polycarbonate resin containing Proprietary Filler(s).This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 2.29 GPa | 332 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp DX93681 PC (Asia Pacific) LNP* Thermocomp* DX93681 is a compound based on Polycarbonate resin containing Proprietary Filler(s).This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 2.29 GPa | 332 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL PVX524 PPE PREVEX* PVX524 resin is a high flow, non FR grade, 100 C HDT |