Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.28 GPa | 330 ksi | ASTM D790 |
Multibase Multi-Pro® 4017 C Polypropylene Calcium Carbonate Filler, 40% by weight.Features:Stiffness, Good Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Flexural Modulus | 2.28 GPa | 330 ksi | ASTM D790 |
Polymer Resources ABS-GP1-[color]-3 ABS, General Purpose, UV-stabilized Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Flexural Modulus | 2.28 GPa | 330 ksi | ASTM D790 |
Polymer Resources PC/ABS-GP1-[color]-UV General Purpose PC/ABS Alloy, UV-stabilized PC/ABS Alloy, General Purpose, UV-stabilized Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provide.. |
|||
Flexural Modulus | 2.28 GPa | 330 ksi | ASTM D790 |
Polymer Resources PC/ABS-GP2 General Purpose PC/ABS Alloy, High Flow PC/ABS Alloy, General Purpose, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by .. |
|||
Flexural Modulus | 2.28 GPa | 330 ksi | ASTM D790 |
Polymer Resources PC/ABS-GP1-[color]-EP General Purpose PC/ABS Alloy, Electroplating Grade PC/ABS Alloy, General Purpose, Electroplating GradeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information p.. |
|||
Flexural Modulus | 2.28 GPa | 330 ksi | ASTM D790 |
Global PC-1408 General Purpose Polycarbonate Information provided by Global Polymers Corporation. |
|||
Flexural Modulus | 2.28 GPa | 330 ksi | ASTM D790 |
Global PC-FR2 UL Recognized 94V-2 Polycarbonate Information provided by Global Polymers Corporation. |
|||
Flexural Modulus | 2.28 GPa | 330 ksi | 2.0 in/min; ASTM D790 |
LTL Color Compounds ColorFast® FRA202 General Purpose ABS General purpose V0/5VA-rated ABSAll information provided by LTL Color Compounders, Inc. |
|||
Flexural Modulus | 2.28 GPa | 330 ksi | ASTM D790 |
LTL Color Compounds ColorRxâ„¢ PC-1000RX Biocompatible Polycarbonate A biocompatible, 10 melt grade of Polycarbonate for healthcare applications.All information provided by LTL Color Compounders, Inc. |
|||
Flexural Modulus | 2.28 GPa | 330 ksi | ASTM D790 |
LTL Color Compounds ColorRxâ„¢ PC-1002AF Food Grade Polycarbonate A biocompatible, 10 melt grade of Polycarbonate for healthcare applications, containing antimicrobial protection.All information provided by LTL Color Compounders, Inc. |
|||
Flexural Modulus | 2.28 GPa | 330 ksi | ASTM D790 |
Spartech Sta-Tuf High Impact Thermoplastic Alloy Sign Grade Sheet Description: Sign Grade SheetInformation provided by Spartech. |
|||
Flexural Modulus | 2.28 GPa | 330 ksi | ASTM D790 |
Star Plastics ABS450FR Molding Grade ABS Information provided by Star Plastics, Inc. |
|||
Flexural Modulus | 2.28 GPa | 330 ksi | ASTM D790 |
Techmer ES HiFill® PC R GY143 Availability: North AmericaForms: PelletsFeatures: Low Smoke EmissionInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 2.28 GPa | 330 ksi | ASTM D790 |
Techmer ES HiFill® POM 0223 B Acetal Availability: North AmericaForms: PelletsFeatures: Copolymer and High Specific GravityInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 2.28 GPa | 330 ksi | ASTM D790 |
Techmer ES Luriblend® PA6/6 TL20 HS L Nylon 66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and PTFE Lubricant(20%)Features: Lubricated, Heat Stabilized and Good Wear ResistanceInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 2.28 GPa | 330 ksi | 0.125 in, injection molded, unannealed; ASTM D790 |
Styron EMERGEâ„¢ 4410-11 MFR Polycarbonate EMERGEâ„¢ PC 4410-11 advanced resin is a high impact polycarbonate resin designed for Information Technology Equipment and Injection Molding Applications.Information provided by DowThis product l.. |
|||
Flexural Modulus | 2.28 GPa | 330 ksi | ASTM D790 |
A. Schulman ComAlloy® E-12672 Polyester Alloy Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 2.28 GPa | 330 ksi | ASTM D790 |
A. Schulman ComAlloy® E-12672 Polyester Alloy Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 2.28 GPa | 330 ksi | Tangent, chs 0.05 in/min; ASTM D790 |
Diamond Polymers ASA S510 Description: ASA Weatherable Polymer, Injection Molding Grade, Medium ImpactInformation provided by Diamond Polymers, Inc. |
|||
Flexural Modulus | 2.28 GPa | 330 ksi | ASTM D-790 |
Axiall UV-6676 Rigid PVC, Molding Georgia Gulf UV-6676 is a weatherable, high flow injection molding compound, specially formulated for outdoor UV exposure. This compound was designed to be used in various accessory parts, such as .. |
|||
Flexural Modulus | 2.28 GPa | 330 ksi | ASTM D790 |
Amco Amalloy® B1017A Clear Multipolymer Alloy Amco Amalloy B1017A is a high impact multipolymer with exceptional clarity, good tensile and flexural strength, and medium-high melt flow.Super high impact, medium melt flow, good tensile and flexur.. |
|||
Flexural Modulus | 2.28 GPa | 330 ksi | ASTM D790 |
Spartech Solarex® K High Heat Weatherable Copolyester Sign Grade Sheet Information provided by Spartech. |
|||
Flexural Modulus | 2.28 GPa | 330 ksi | ASTM D790 |
Amco Amalloy® B9941 Polymer Alloy Amco Amalloy B9941 is a clear performance copolymer with exceptional clarity and toughness.Good flexural and tensile strength.Information provided by Amco Plastic Materials. |