Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.16 GPa | 313 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® HPS2S PC (Asia Pacific) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma steriliza.. |
|||
Flexural Modulus | 2.16 GPa | 313 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® EXRL2032 PC (Asia Pacific) Lexan EXRL2032 is a flame retardant transparent polycarbonate featuring non brominated and non chlorinated FR system with good flow and thin wall FR performance. It intended to meet WEEE/RoHS requir.. |
|||
Flexural Modulus | 2.16 GPa @Thickness 3.20 mm |
313 ksi @Thickness 0.126 in |
15mm/min; ASTM D790 |
LG Chemical HIPS 460AF PS, Flame Retardant Description: Injection Molding, PS, Flame RetardantApplication: Electric Parts Requiring Flame RetardancyCAS: 9003-55-8, 25713-60-4, 84852-53-9 and 1309-64-4Information provided by LG Chemical |
|||
Flexural Modulus | 2.16 GPa @Thickness 3.20 mm |
313 ksi @Thickness 0.126 in |
15mm/min; ASTM D790 |
LG Chemical LUCON TR1000 PMMA+CNT Description: Injection Molding, PMMA+CNT, Transparency, Permanent Antistatic, Low OutgassingApplication: Wafer Carrier Cover, Pellicle TrayCAS No. 9010-94-0 and 25053-09-2Information provided by LG .. |
|||
Flexural Modulus | 2.16 GPa @Thickness 6.40 mm |
313 ksi @Thickness 0.252 in |
2.5mm/min; ASTM D790 |
LG Chemical Lupox® TE5000HZ PBT+PC Description: Injection Molding, PBT+PC, High Impact, Dimensional StabilityApplication: Automotive (Door Handle)CAS No. 9003-01-04, 24968-12-5 and 103598-77-2Information provided by LG Chemical |
|||
Flexural Modulus | 2.16 GPa | 313 ksi | ASTM D790 |
Kotec Carbotex K-40UVR Polycarbonate, General Purpose, UV Stability + Mold Release Grade Features: UV stability, Mold release, Medium viscosityApplications: OA equipment, Communications, Precision parts, Machineries, Lighting fixtures, Safety products, E & E parts, Household application.. |
|||
Flexural Modulus | 2.16 GPa | 313 ksi | ASTM D790 |
Kotec Carbotex K-50UVR Polycarbonate, General Purpose, UV Stability + Mold Release Grade Features: UV stability, Mold release, Medium viscosityApplications: OA equipment, Communications, Precision parts, Machineries, Lighting fixtures, Safety products, E & E parts, Household application.. |
|||
Flexural Modulus | 2.16 GPa | 313 ksi | 5 mm/min; ISO 178 |
Gromax BTG25-FN09N1 Nylon 6 25% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Flexural Modulus | 2.16 GPa @Thickness 3.20 mm |
313 ksi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical MA221 ABS, High Impact, Low Gloss Feature: Injection Molding, Extrusion Molding, High Impact, Low GlossApplication: Automotive Sheet, Semi-Conductor TrayCAS No. 9003-56-9Information provided by LG Chemical |
|||
Flexural Modulus | 2.16 GPa | 313 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRILOY KL201 Acetal LNP LUBRILOY* KL201 is a compound based on Acetal resin containing Proprietary Lubricant. PTFE. Added feature of this material is: Wear Resistant. |
|||
Flexural Modulus | 2.16 GPa | 313 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® HI-1001BG PC/ABS, Metal Plating Grade PC/ABS material that can be used in automobile wheel cap and air-conditioner panelInformation provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.16 GPa | 313 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® HR-0370F ABS, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.16 GPa | 313 ksi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® VH-0800 ABS, Unreinforced FR Flame-retardant ABS with excellent weather resistance that is used in the exterior of OA devices such as monitors, printers, fax machines, duplicators etc.Information provided by Samsung Cheil Indus.. |
|||
Flexural Modulus | 2.16 GPa | 313 ksi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® VH-0819 ABS, Unreinforced FR Flame-retardant high flow ABS that can be used for the exterior of large TV and OA devicesInformation provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.16 GPa | 313 ksi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® WX-9300 ASA, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.16 GPa | 313 ksi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® WX-9300UV ASA, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.16 GPa | 313 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® BC-0130 X ABS, Unreinforced General Purpose Stiff ABS material that is used for battery casesInformation provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.16 GPa | 313 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® SR-0315 V ABS, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.16 GPa | 313 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® SR-0320 K ABS, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.16 GPa | 313 ksi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® VH-0819 ABS, Unreinforced FR Flame-retardant high flow ABS that can be used for the exterior of large TV and OA devicesInformation provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.16 GPa | 313 ksi | ASTM D790 |
Samyang Trirex® 3020IR Polycarbonate with Heat Stabilizer PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3020IR is a high flow grade with added heat stabilizers, separating materials and stain.. |
|||
Flexural Modulus | 2.16 GPa | 313 ksi | ASTM D790 |
Shinkong Synthetic Fibers Shinite® P301T20 PP, 20% Talc Filled Information from Shinkong Synthetic Fibers Corp. |
|||
Flexural Modulus | 2.16 GPa @Thickness 3.20 mm |
313 ksi @Thickness 0.126 in |
ASTM D790 |
Supreme Petrochem SP 253 Toughened Polystyrene Characteristics High rigidity Improved toughness Good clarityProcessing Injection moldingApplications Ball pens Small appliances housings Small impellersMaterial Status: Commercial : ActiveAgenc.. |
|||
Flexural Modulus | 2.16 GPa | 313 ksi | 23°C, 50% RH; ASTM D790 |
Asahi Kasei Xyron® X5402 PPE/PA Oil ResistantInformation provided by Asahi Kasei |
|||
Flexural Modulus | 2.16 GPa @Thickness 6.40 mm |
313 ksi @Thickness 0.252 in |
5 mm/min; ASTM D790 |
Bhansali Engineering Abstron HI40I ABS Injection Molding Grade Automotive applications -Super High Impact , High Rigidity, PaintableInformation provided by Bhansali |
|||
Flexural Modulus | 2.16 GPa @Thickness 6.40 mm |
313 ksi @Thickness 0.252 in |
5 mm/min; ASTM D790 |
Bhansali Engineering Abstron KU602M ABS Heat Resistant High rigidityInformation provided by Bhansali |
|||
Flexural Modulus | 2.16 GPa @Thickness 6.40 mm |
313 ksi @Thickness 0.252 in |
5 mm/min; ASTM D790 |
Bhansali Engineering Abstron KU603 ABS Heat Resistant High Impact, High RigidityInformation provided by Bhansali |
|||
Flexural Modulus | 2.16 GPa @Thickness 6.40 mm |
313 ksi @Thickness 0.252 in |
ASTM D-790 |
Bhansali Engineering Abstron IM-17A(HF) ABS Injection Molding Grade Very High Flow, Medium Impact GradeInformation provided by Bhansali |
|||
Flexural Modulus | 2.16 GPa @Thickness 3.20 mm |
313 ksi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY NS5000C PC/ABS, High Impact Description: Injection Molding, PC/ABS, Heat Resistance, High Flow, High ImpactApplication: Automotive (Interior)CAS: 103598-77-2 and 9003-56-9Information provided by LG Chemical |
|||
Flexural Modulus | 2.16 GPa | 313 ksi | ASTM D790 |
SABIC Innovative Plastics NORYL PX2622 PPE+HIPS (Asia Pacific) PPE/HIPS for auto interior |