Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 21.4 GPa | 3100 ksi | ASTM D790 |
LATI LARPEEK 10 K/30 30% Carbon Fiber Reinforced Polyetheretherketone (PEEK)
(Unverified Data**) Larpeek polyetheretherketone (PEEK) is a high performance thermoplastic offering cost effective performance in difficult environments across all industries. PEEK is temperature resistant (up to 250°.. |
|||
Flexural Modulus | 21.4 GPa | 3100 ksi | ASTM D790 |
Techmer ES HiFill® PA4/6 CF40 HS 40% Carbon Filled (Conditioned) Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 40% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedInformation provided by TP Composites.. |
|||
Flexural Modulus | 21.4 GPa | 3100 ksi | ASTM D790 |
Techmer ES HiFill® PA6/6 LGF60 HS L BK 12 mm Availability: North AmericaForms: PelletsFiller/Reinforcement: Long Glass FiberAdditive: Lubricant and Heat StabilizerFeatures: Lubricated, Heat Stabilized and Good MoldabilityAppearance: BlackProce.. |
|||
Flexural Modulus | 21.4 GPa | 3100 ksi | ASTM D790 |
Techmer ES HiFill® PA6/6 LGF60 HS L BK 12 mm Availability: North AmericaForms: PelletsFiller/Reinforcement: Long Glass FiberAdditive: Lubricant, UV Stabilized and Heat StabilizerFeatures: Lubricated and Heat StabilizedProcessing Method: Inject.. |