Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.212 GPa | 30.7 ksi | ASTM D790 |
NOVA Chemicals Novapol® LF-0219-A LDPE Blow Molding Resin Good heat sealing latitude, Easy processabilityApplications: Food contact, Squeeze bottles, Non-ESCRAdditives: Base resinInformation provided by NOVA Chemicals. |
|||
Flexural Modulus | 0.212 GPa | 30.7 ksi | ASTM D790 |
LyondellBasell Petrothene® NA205000 Low Density Polyethylene, Extrusion Coating Grade Petrothene NA205000 is an extrusion coating resin especially recommended for high-speed, light weight coating applications. The resin can be drawn to a low coating weight at line speeds in excess of.. |
|||
Flexural Modulus | 0.212 GPa | 30.7 ksi | Conditioned 15 days at 23°C - 50% RH; ISO178 |
Arkema Group Pebax® Clear 300 Polyether Block Amide (PEBA) Pebax® Clear 300 combines high transparency level with the unique performance of Pebax®, thermoplastic elastomer made of flexible polyether and rigid polyamide.Information provided by Arkema Group.. |