Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.067 GPa | 299.8 ksi | tangent; chs 0.05 in/min; ASTM D790 |
Diamond Polymers ABS 3500 ELG Natural 1003 Injection Molding Grade, High Flow, Medium Impact, Low Gloss Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Flexural Modulus | 2.067 GPa | 299.8 ksi | tangent; chs 0.05 in/min; ASTM D790 |
Diamond Polymers ABS 3500 Natural 1003 Injection Molding Grade, High Flow, Medium Impact, Low Gloss Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Flexural Modulus | 2.067 GPa | 299.8 ksi | chs 0.05 in/min; ASTM D790 |
Diamond Polymers ASAPC 122954H Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Flexural Modulus | 2.067 GPa | 299.8 ksi | tangent; chs 0.05 in/min; ASTM D790 |
Diamond Polymers Centrex® HGM Automotive Grade, Injection Molding Grade Centrex HGM resin is an exceptionally high-gloss grade of ASA (acrylonitrile-styrene-acrylate). This injection molding grade has excellent gloss retention, excellent resistance to chemicals and high.. |