Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.05 GPa | 297 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® CY100FC PC+ABS (Asia Pacific) High impact PC+ABS material designed for local Pacific Automotive applications |
|||
Flexural Modulus | 2.05 GPa | 297 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® BFL4000U PC (Asia Pacific) Lexan* BFL4000U Polycarbonate resin is an injection moldable grade. It contains non-brominated, non-chlorinated flame retardant systems with UL-94 V0 rating and good impact/flow balance. Designed fo.. |
|||
Flexural Modulus | 2.05 GPa | 297 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® FXE1414L PC Copolymer Opaque EXL, UV-Stabilized & light shielding capability (Wall thickness >0.8mm), for portable electronics device enclosure application. Only available in white, grey and limited pastel colors. Consul.. |
|||
Flexural Modulus | 2.05 GPa | 297 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® FXE1414L PC Copolymer (Asia Pacific) Opaque EXL, UV-Stabilized & light shielding capability (Wall thickness >0.8mm), for portable electronics device enclosure application. Only available in white, grey and limited pastel colors. Consul.. |
|||
Flexural Modulus | 2.05 GPa | 297 ksi | ISO 178 |
Total Lacqrene® 1235 High Impact Polystyrene
(discontinued **) LACQRENE® 1235 is a high gloss, high impact polystyrene used in injection molding and co-extrusion. This grade produces articles with a surface gloss level equivalent to that of certain grades of .. |
|||
Flexural Modulus | 2.05 GPa @Temperature 90.0 °C |
297 ksi @Temperature 194 °F |
ISO 178, ASTM D790 |
Nilit Nilamid B3 H G3 15% Glass Fiber Reinforced PA6 Description: Nilamid B3 H G3 is a general purpose, 15% glass fiber reinforced NYLON 6. These products combine good overall mechanical performance and impact strength with ease of processing. Key cha.. |
|||
Flexural Modulus | 2.05 GPa | 297 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® BFL4000U PC Lexan* BFL4000U Polycarbonate resin is an injection moldable grade. It contains non-brominated, non-chlorinated flame retardant systems with UL-94 V0 rating and good impact/flow balance. Designed fo.. |
|||
Flexural Modulus | 2.05 GPa | 297 ksi | 2 mm/min; ISO 178 |
Inno-Comp INNOPOL® CS 3-9230 KAR YU UV-Stabilized, 26% Mineral-Filled Compound Blend Of Polypropylene Homopolymer And Block-Copolymer INNOPOL® CS 3-9230 KAR YU is a yellow colored, UV-stabilized, 26% mineral-filled compound based on a blend of polypropylene homopolymer and block-copolymer.INNOPOL® CS 3-9230 KAR YU is develop.. |
|||
Flexural Modulus | 2.05 GPa | 297 ksi | ASTM D790 |
SABIC Innovative Plastics NORYL STN15 PPE+HIPS (Asia Pacific) PPE+HIPS Unfilled Auto Interior |
|||
Flexural Modulus | 2.05 GPa | 297 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® IQ357 PBT+PC Valox* Resin IQ357: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified. |
|||
Flexural Modulus | 2.05 GPa | 297 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® IQ357M PBT+PC (Asia Pacific) Valox* Resin IQ357M: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified, easy flow product with mold release. |
|||
Flexural Modulus | 2.05 GPa | 297 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® IQ357U PBT+PC Valox* Resin IQ357U: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified and UV stabilized resin. |
|||
Flexural Modulus | 2.05 GPa | 297 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Xenoy® CL100 PBT+PC Xenoy CL100 is an unfilled, impact modified, UV-stabilized PC/PBT blend with excellent solvent resistance and good low-temperature ductility. It has a proven track record in unpainted exterior autom.. |
|||
Flexural Modulus | 2.05 GPa | 297 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Xenoy® CL100 PBT+PC (Asia Pacific) Xenoy CL100 is an unfilled, impact modified, UV-stabilized PC/PBT blend with excellent solvent resistance and good low-temperature ductility. It has a proven track record in unpainted exterior autom.. |
|||
Flexural Modulus | 2.05 GPa | 297 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Xenoy® CL100 PBT+PC (Asia Pacific) Xenoy CL100 is an unfilled, impact modified, UV-stabilized PC/PBT blend with excellent solvent resistance and good low-temperature ductility. It has a proven track record in unpainted exterior autom.. |
|||
Flexural Modulus | 2.05 GPa | 297 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Xenoy® CL100 PBT+PC (Europe-Africa-Middle East) Xenoy CL100 is an unfilled, impact modified, UV-stabilized PC/PBT blend with excellent solvent resistance and good low-temperature ductility. It has a proven track record in unpainted exterior autom.. |
|||
Flexural Modulus | 2.05 GPa | 297 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Xenoy® CL100 PBT+PC (Europe-Africa-Middle East) Xenoy CL100 is an unfilled, impact modified, UV-stabilized PC/PBT blend with excellent solvent resistance and good low-temperature ductility. It has a proven track record in unpainted exterior autom.. |
|||
Flexural Modulus | 2.05 GPa | 297 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Xenoy® HX5600HP PBT+PC (Asia Pacific) Xenoy HX5600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing.. |
|||
Flexural Modulus | 2.05 GPa | 297 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Xenoy® X5100 PC+PBT (Europe-Africa-Middle East) XENOY X5100 is a semi-crystalline, impact modified PC-PBT blend with excellent flow. (PC+PBT-I). |
|||
Flexural Modulus | 2.05 GPa | 297 ksi | ASTM Test |
Styrolution Terluran® HI-10 ABS Terluran HI-10 is an injection molding and extrusion grade of ABS with very high toughness and medium flow.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Flexural Modulus | 2.05 GPa | 297 ksi | 3-point, 2 mm/min; ISO 178 |
Styron MAGNUMâ„¢ 3416 SLG Acrylonitrile Butadiene Styrene (ABS) Resin Overview: The mass (continuous process) ABS technology of Styron ensures an ABS resin that combines excellent processability with a stable light base color providing an ideal resin for self coloring.. |
|||
Flexural Modulus | 2.05 GPa | 297 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Noryl GTX GTX979 PPE+PA NORYL GTX979 is a conductive, high heat material. It is especially designed for in- and on-line painted bodypanels and fenders in particular, with conductivity for electro-static painting in an uniq.. |
|||
Flexural Modulus | 2.05 GPa | 297 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Noryl GTX GTX979 PPE+PA (Asia Pacific) NORYL GTX979 is a conductive, high heat material. It is especially designed for in- and on-line painted bodypanels and fenders in particular, with conductivity for electro-static painting in an uniq.. |
|||
Flexural Modulus | 2.05 GPa | 297 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL NWP100 PPE+HIPS (Asia Pacific) PPO/HIPS Unfilled high impact extrusion grade |
|||
Flexural Modulus | 2.05 GPa | 297 ksi | ASTM D 790 |
SABIC Innovative Plastics Noryl EUN0240 PPE+HIPS (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 2.05 GPa | 297 ksi | ASTM D790 |
SABIC Innovative Plastics NORYL GTX GTX600 PPE+PA6 (Asia Pacific) Pa6 based unfilled GTX |
|||
Flexural Modulus | 2.05 GPa | 297 ksi | ISO 178 |
Polyplastics Duracon® WR-01 Acetal Co-polymer (POM), Chlorine water resistance DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Flexural Modulus | 2.05 GPa | 297 ksi | ISO 178 |
Eurostar Star L POM D51 POM, Injection Molded Star L POM D51 is a PTFE Lubricated, POM Copolymer Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Modulus | 2.05 GPa | 297 ksi | DAM; ISO 178 |
DuPont Performance Polymers Zytel® 158L NC010 Nylon 612
(Unverified Data**) Unreinforced Polyamide 612Information provided by DuPont Performance Polymers |
|||
Flexural Modulus | 2.05 GPa | 297 ksi | ASTM D 790 |
SABIC Innovative Plastics Noryl EUN1240 PPE+HIPS (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |