Polymer Property : Flexural Modulus = 292.3 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 2.015 GPa
292.3 ksi
2 mm/min; ISO 178
Nyco NYGLOS® 4W STO105 Wollastonite in Polypropylene
Data for polypropylene reinforced with 15% Nyco NYGLOS® 4W STO105 Wollastonite. Polypropylene used is Braskem TI6200Q High Impact Copolymer 20 MFR -NBWollastonite (calcium metasilicate, or CaSiO3)..
Flexural Modulus 2.015 GPa

@Temperature 23.0 °C
292.3 ksi

@Temperature 73.4 °F
ISO 178
DuPont Performance Polymers Crastin® CE2056 NC010 PBT
Crastin® CE2056 NC010 is an unreinforced polybutylene terephthalate molding resin.Information provided by DuPont Performance Polymers