Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 19.3 GPa @Temperature 23.9 °C |
2800 ksi @Temperature 75.0 °F |
Dry; 8HS form; ASTM D790 |
Park Electrochemical Nelcote® F-555 Phenolic Prepreg, ENKA Reinforced Nelcote® F-555 is a carbon-filled MIL-R-9299 phenolic resin optimized for coating Carbonized Rayon cloth. F-555 is used extensively in the manufacture of high temperature rocket nozzles, heat shiel.. |
|||
Flexural Modulus | 19.3 GPa | 2800 ksi | ASTM D790 |
Solvay Specialty Polymers AvaSpire® AV-722 CF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-722 CF30 is a 30% carbon fiber reinforced version of AvaSpire AV-722. This formulation offers improved part economics relative to 30% carbon fiber reinforced PEEK while retaining most of.. |
|||
Flexural Modulus | 19.3 GPa | 2800 ksi | ASTM D790 |
Solvay Specialty Polymers Ryton® BR111BL Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® BR111BL Ryton® BR111 is a black-colored glass fiber and mineral filled polyphenylene sulfide compound that provides enhanced mechanical strength with good electrical properties and outs.. |
|||
Flexural Modulus | 19.3 GPa | 2800 ksi | ASTM D790 |
Solvay Specialty Polymers Ryton® R-7-120BL Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® R-7-120NA and R-7-120BL glass fiber and mineral filled polyphenylene sulfide compounds provide good strength and low maintenance molding using conventional molding equipment.Features: Good.. |
|||
Flexural Modulus | 19.3 GPa | 2800 ksi | ASTM D790 |
Solvay Specialty Polymers Ryton® R-7-120NA Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® R-7-120NA and R-7-120BL glass fiber and mineral filled polyphenylene sulfide compounds provide good strength and low maintenance molding using conventional molding equipment.Features: Good.. |
|||
Flexural Modulus | 19.3 GPa | 2800 ksi | ASTM D790 |
Solvay Specialty Polymers Ryton® R-7-220BL Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® R-7-220BL glass fiber and mineral filled polyphenylene sulfide compound provides enhanced mechanical strength after constant or repeated exposure to high temperature water.Features: Good S.. |
|||
Flexural Modulus | 19.3 GPa | 2800 ksi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF55 HS L 55% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 55% Filler by WeighAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedUL File Nu.. |
|||
Flexural Modulus | 19.3 GPa | 2800 ksi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF55 HS L BK 55% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 55% Filler by WeighAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedUL File Nu.. |
|||
Flexural Modulus | 19.3 GPa | 2800 ksi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF55 HS L OR016 57% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 57% Filler by WeighAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedUL File Nu.. |
|||
Flexural Modulus | 19.3 GPa | 2800 ksi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF55 L BK 55% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 55% Filler by WeighAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedUL File Nu.. |
|||
Flexural Modulus | 19.3 GPa | 2800 ksi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF60 HS L BK 60% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedUL File N.. |
|||
Flexural Modulus | 19.3 GPa | 2800 ksi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF60 X 60% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedUL File N.. |
|||
Flexural Modulus | 19.3 GPa | 2800 ksi | ASTM D790 |
Techmer ES Plastiblend® PC/PBT IM 5727 BK Availability: North AmericaForms: PelletsAdditive: Impact Modifier and UV StabilizerFeatures: Impact ModifiedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 19.3 GPa | 2800 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp RF00CS PA 66 LNP* Thermocomp* RF00CS is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Americas re.. |
|||
Flexural Modulus | 19.3 GPa | 2800 ksi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF60 HS L 60% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedUL File N.. |
|||
Flexural Modulus | 19.3 GPa | 2800 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP RF00CSXZ PA 66 LNP* THERMOCOMP* RF00CSXZ is a compound based on Recycled Nylon 66 resin containing 60% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Flexural Modulus | 19.3 GPa | 2800 ksi | ASTM D790 |
SABIC Innovative Plastics LNP VERTON UF-700-12 HS EXP PPA (Asia Pacific) LNP* Verton* UF-700-12 HS EXP is a compound based on Polyphthalamide resin containing Long Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Flexural Modulus | 19.3 GPa | 2800 ksi | ASTM D790 |
Techmer ES Electrablend® ABS CF40 BK 40% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 40% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 19.3 GPa | 2800 ksi | ASTM D790 |
PolyOne Edgetek® PI-40CF/000 Polyetherimide (PEI), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |