Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.900 GPa | 275.6 ksi | 1% tangent, 0.05 in/min.; LAB033 |
ExxonMobil Mytex™ AS23K(W)-01 Talc filled compounded polypropylene produced for automotive interior applicationsInformation provided by ExxonMobil Chemical |