Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 18.95 GPa | 2748 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP RCL26 PA6.6 LNP* LUBRICOMP* RCL26 is a compound based on Nylon 66 containing 30% Carbon Fiber, 10% PTFE. Added features of this grade include: Wear Resistant, Electrically Conductive. |