Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.88 GPa | 273 ksi | 1.3 mm/min; ASTM D790 |
PolyOne LubriOne™ AT-000/10T 2S Acetal (POM) Copolymer LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Flexural Modulus | 1.88 GPa | 273 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Geloy XTWE265 ASA Highly weatherable Geloy ASA profile extrusion grade for processes with simple or no calibration hardware.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 1.88 GPa | 273 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics GELOY XTWE265 ASA (Asia Pacific) Highly weatherable Geloy ASA profile extrusion grade for processes with simple or no calibration hardware. |
|||
Flexural Modulus | 1.88 GPa | 273 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Geloy XTWE265 ASA (Europe-Africa-Middle East) Highly weatherable Geloy ASA profile extrusion grade for processes with simple or no calibration hardware.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Modulus | 1.88 GPa | 273 ksi | ASTM D790 |
Metton LMR M1534 Liquid Molding Resin Different product numbers represent different formulations for customer specific needs such as liquid freezing point. Metton LMR is a tough and durable engineering plastic material used to produce .. |
|||
Flexural Modulus | 1.88 GPa | 273 ksi | |
Kraton® G1654 + PPE blend (20/80) Unmodified polypropylene has high rigidity and good heat resistance, but poor impact resistance, especially at low temperatures. Blending KRATON D and G polymers with PPE significantly improves the.. |
|||
Flexural Modulus | 1.88 GPa | 273 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-LOY NX13401 PC+ABS LNP* STAT-LOY* NX13401 is a compound based on PC+ABS blend. Added features of this material include: Antistat, Flame Retardant, Excellent Release. |
|||
Flexural Modulus | 1.88 GPa | 273 ksi | Tangent, chs 0.05 in/min; ASTM D790 |
Diamond Polymers ASA S190 Description: ASA Weatherable Polymer, Injection Molding Grade, Very High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Flexural Modulus | 1.88 GPa | 273 ksi | Tangent, chs 0.05 in/min; ASTM D790 |
Diamond Polymers ASA S750 Description: ASA Weatherable Polymer, Injection Molding Grade, Very High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Flexural Modulus | 1.88 GPa | 273 ksi | Tangent, chs 0.05 in/min; ASTM D790 |
Diamond Polymers ASA S910 Description: ASA Weatherable Polymer, Injection Molding Grade, Very High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Flexural Modulus | 1.88 GPa | 273 ksi | parallel; ASTM D790 |
Dow SPECTRIM™ HH 390 Reaction Moldable Polymer Information provided by Dow |
|||
Flexural Modulus | 1.88 GPa | 273 ksi | ASTM D790 |
Entec Hyrene® PS-HI 3/2 High Impact Polystyrene Available in North America Features: High Impact ResistanceRoHS Compliant Form: Pellets Information provided by Entec |
|||
Flexural Modulus | 1.88 - 11.4 GPa | 273 - 1650 ksi | Average value: 4.43 GPa Grade Count:104 |
Overview of materials for Polypropylene, Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum .. |