Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.87 GPa | 271 ksi | ASTM D790 |
PolyOne Nymax™ 2024 HS UV 425C Grey Polyamide 66 (Nylon 66) The Nymax® Series of nylon 6/6 compounds have been specifically developed to deliver outstanding performance in a wide range of application areas. These materials are available with a broad range o.. |
|||
Flexural Modulus | 1.87 GPa | 271 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Geloy XTWE270M ASA+SAN (Asia Pacific) Excellent weatherability, good flow/aesthetics and good impact.Profile co-extrusion grade over ABS, PVC or other compatible polymers. XTWE270M is available in various colours.This data was supplied.. |
|||
Flexural Modulus | 1.87 GPa | 271 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Lubricomp IP003 PA6.12 LNP* Lubricomp* IP003 is a Nylon 6/12 base resin containing PTFE and Silicone.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 1.87 GPa | 271 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® V2105U PBT Unreinforced, Wear resistant, UV Stabilized PBT designed for outdoor, agricultural, industrial and automotive applications. This grade has very high impact strength to stiffness ratio. |
|||
Flexural Modulus | 1.87 GPa | 271 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® V2105U PBT (Europe-Africa-Middle East) Unreinforced, Wear resistant, UV Stabilized PBT designed for outdoor, agricultural, industrial and automotive applications. This grade has very high impact strength to stiffness ratio. |
|||
Flexural Modulus | 1.87 GPa @Thickness 19.0 mm |
271 ksi @Thickness 0.750 in |
ASTM D790 |
3A Composites Core Materials AIREX® PXw.320 Fiber-Reinforced Structural Foam Panel AIREX® PXw is a closed-cell, fiber reinforced polymer foam panel with a special formulation and very high mechanical properties. The sophisticated manufacturing process evenly distributes continuou.. |
|||
Flexural Modulus | 1.87 GPa | 271 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® V2105U PBT (Asia Pacific) Unreinforced, Wear resistant, UV Stabilized PBT designed for outdoor, agricultural, industrial and automotive applications. This grade has very high impact strength to stiffness ratio. |