Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 18.6 GPa | 2700 ksi | 1.3 mm/min; ASTM D790 |
Ovation Polymers Nemcon™ E PK DP104 Polyetheretherketone, Carbon Fiber Reinforced Nemcon™ E PK DP104 is a carbon fiber reinforced polyetheretherketone, characterized by high strength, stiffness, consistent moldabiliity, and exceptional thermal resistance.All properties after 48h.. |
|||
Flexural Modulus | 18.6 GPa @Temperature 23.9 °C |
2700 ksi @Temperature 75.0 °F |
Dry; ASTM D790 |
Park Electrochemical Nelcote® S-860 Silicone Prepreg, 1581-112NPH E-Glass Reinforced Nelcote® S-860 is a MIL-P-25518 type silicone resin with a good combination of electrical and high temperature properties. GMS4001 qualified specificationsKey Features and Benefits:500°F maximum s.. |
|||
Flexural Modulus | 18.6 GPa | 2700 ksi | Lengthwise; ASTM D790 |
G-10 Fiberglass Epoxy Laminate Sheet This glass-epoxy laminate is specified for its extremely high strength and high dimensional stability over temperature. G-10 is used for terminal boards, high humidity applications, electrical and e.. |
|||
Flexural Modulus | 18.6 GPa | 2700 ksi | Crosswise; ASTM D790 |
G-11 Fiberglass Epoxy Laminate Sheet This glass-epoxy laminate is specified for its extremely high strength and high dimensional stability over temperature. G-11 is used for terminal boards, high humidity applications, electrical and e.. |
|||
Flexural Modulus | 18.6 GPa | 2700 ksi | ASTM D790 |
Solvay Specialty Polymers Amodel® AS-1566 HS Polyphthalamide (PPA), 65% GlassMineral (Dry) Amodel® AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin that exhibits a high deflection temperature and high flexural modulus. This grade was designed specifica.. |
|||
Flexural Modulus | 18.6 GPa | 2700 ksi | ASTM D790 |
Techmer ES Electrafil® J-1/CF/30 Nylon 66, 30% Carbon Fiber Reinforced Carbon Fiber Reinforced |
|||
Flexural Modulus | 18.6 GPa | 2700 ksi | ASTM D790 |
Techmer ES HiFill® PEEK CF20 TL15 HF 20% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 20% Filler by WeightAdditive: LubricantFeatures: High Flow and LubricatedInformation provided by TP Composi.. |
|||
Flexural Modulus | 18.6 GPa | 2700 ksi | ASTM D790 |
Techmer ES Luriblend® PA6/6 CF30 TL12 30% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAdditive: PTFE + Silicone Lubricant(15%)Features: Lubricated and Good Wear ResistanceTPCI# 6466101Inf.. |
|||
Flexural Modulus | 18.6 GPa | 2700 ksi | GB/T 9341-2008 |
Sichuan Deyang Haton® hGR515 Polyphenylene Sulfide/PA Alloy Injection molding, high strengthInformation provided by Sichuan Deyang Chemical Co., LTD |
|||
Flexural Modulus | 18.6 GPa | 2700 ksi | ASTM D790 |
Techmer ES HiFill® PA4/6 CF40 IM HS 40% Carbon Filled (Conditioned) Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 40% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedInformation provided by TP Composites.. |
|||
Flexural Modulus | 18.6 GPa | 2700 ksi | ISO 178 |
Unitika E-RUNG60 PA66, 60% Glass Fiber Reinforced, Dry Information provided by Unitika Ltd. |
|||
Flexural Modulus | 18.6 GPa | 2700 ksi | 45° stress angle |
Cytec Cyply® 1002 Epoxy Fiberglass Composite, Isotropic CYPLY® 1002 is a cured epoxy composite material based on a unique non-woven parallel filament construction. This type of construction minimizes filament stress abrasion that can shorten fatigue li.. |
|||
Flexural Modulus | 18.6 GPa | 2700 ksi | ASTM D790 |
PolyOne Edgetek® PF-40CF/000 Polysulfone, Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 18.6 GPa | 2700 ksi | ASTM D790 |
Solvay Specialty Polymers Amodel® AS-1566 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin that exhibits a high deflection temperature and high flexural modulus. This grade was designed specifically .. |