Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.183 GPa | 26.5 ksi | ASTM D790 |
DuPont 20 Series 2010 Specialty Polyethylene Resin DuPont 2010 specialty low density polyethylene resin is characterized by low melt index and intermediate crystallinity. This product, produced via a unique polymerization process, has outstanding fl.. |