Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.72 - 3.10 GPa | 249 - 450 ksi | ASTM D790 |
PolyOne Stat-Tech™ PC-CB2/000 CR Polycarbonate (PC) Stat-Tech™ PC-CB2/000 CR XP100827Information provided by PolyOne |
|||
Flexural Modulus | 1.72 GPa | 249 ksi | 13 mm/min; ASTM D790 |
PolyOne Edgetek® XT X XT 1000 Natural Copolyester Edgetek™ XT high performance blends offer outstanding strength, durability and chemical resistance through the combination of Eastman Tritan™ copolyester with other various polymeric resins. Edget.. |
|||
Flexural Modulus | 1.72 GPa | 249 ksi | ASTM D790 |
Petromont 3000 High Density Polyethylene Resin Petromont HDPE 3000 is a high density polyethylene resin produced using the UNIPOL® Process. This resin is designed for injection moulding applications such as crates, cases, trays, tote bins and o.. |
|||
Flexural Modulus | 1.72 GPa | 249 ksi | ASTM D790 |
PolyOne Edgetek® XT XT-500-CX02 PC+PBT
(discontinued **) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |
|||
Flexural Modulus | 1.72 GPa | 249 ksi | ASTM D790 |
PolyOne Lubri-Tech™ PS-000/20T Polyester (PBT) - 20% PTFE Lubricated
(discontinued **) Data provided by PolyOne. |
|||
Flexural Modulus | 1.72 GPa @Temperature 100 °C |
249 ksi @Temperature 212 °F |
ISO 178 |
Solvay Specialty Polymers Amodel® AT-1002 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AT-1002 HS is a neat, toughened, heat stabilized polyphthalamide (PPA) resin that offers superior retention of properties after humid thermal aging; high impact at low temperature and better .. |
|||
Flexural Modulus | 1.72 GPa | 249 ksi | ASTM D790 |
PTS Trimid® N66-S100L High Impact Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Modulus | 1.72 GPa | 249 ksi | ASTM D790M |
DSM Somos® WaterClear® 10110 Epoxy Resin for Stereolithography
(discontinued **) DescriptionDSM Somos® 10110 is a high-speed liquid photopolymer that produces strong, rigid, and durable parts with optical clarity using stereolithography machines. This material is especially us.. |
|||
Flexural Modulus | 1.72 GPa | 249 ksi | ASTM D790 |
Hyosung Topilene HJ640A PP HJ640A Impact CopolymerApplications:CompoundingElectric applianceAutomobile partsCharacteristics:High stiffnessHeat resistanceMedium impactInformation provided by Hyosung Corporation |
|||
Flexural Modulus | 1.72 GPa | 249 ksi | ASTM D790 |
Hyosung Topilene HJ740 PP HJ740 High Isostatic PP Impact CopolymerApplications:CompoundingElectric applianceAutomobile partsCharacteristics:High stiffnessHeat resistanceMedium impactInformation provided by Hyosung Corporatio.. |
|||
Flexural Modulus | 1.72 GPa | 249 ksi | ASTM D790 |
LG Chemical LUCEL HI-515 High Impact POM, Unreinforced LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Flexural Modulus | 1.72 GPa | 249 ksi | ASTM D760 |
LG Chemical SEETEC M1315 Polypropylene Impact Copolymer Features: SEETEC M1315 is a heterophasic polypropylene copolymer for compression molding caps, especially SACMI machines. SEETEC M1315 exhibits an excellent stiffness, a high impact strength, a high.. |
|||
Flexural Modulus | 1.72 GPa | 249 ksi | 1% secant; ASTM D790-02 |
Ipiranga Petrochem PH 0130 Polypropylene The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr.. |
|||
Flexural Modulus | 1.72 GPa | 249 ksi | 1% secant; ASTM D790-02 |
Ipiranga Petrochem PH 0130 Polypropylene The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr.. |
|||
Flexural Modulus | 1.72 GPa | 249 ksi | ASTM D790B |
Lotte Chemical Titan TITANPRO® 6331 Polypropylene homopolymer The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (c)1.1a. The adjuvants meet their respective FDA regulations and 21 CFR 1.. |
|||
Flexural Modulus | 1.72 GPa | 249 ksi | ASTM D790B |
Lotte Chemical Titan TITANPRO® PM655 Polypropylene homopolymer The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (c)1.1a. The adjuvants meet their respective FDA regulations and 21 CFR 1.. |
|||
Flexural Modulus | 1.72 GPa | 249 ksi | ASTM D790 |
Gromax PBT 2100-104B Product Description: PBT unreinforced flame-retarded injection molding grade. Characteristics:Excellent electrical property Excellent mechanic and chemical property Excellent weatherability Excellen.. |
|||
Flexural Modulus | 1.72 GPa | 249 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP ML004LS PP LNP* LUBRICOMP* ML004LS is a compound based on Polypropylene resin containing 20% PTFE. Added features of this matLNP* Lubricomp* ML004LS is a compound based on Polypropylene resin containing PTFE... |
|||
Flexural Modulus | 1.72 GPa @Temperature 100 °C |
249 ksi @Temperature 212 °F |
ISO 178 |
Solvay Specialty Polymers Amodel® AT-1002 HS Polyphthalamide (PPA) Amodel® AT-1002 HS is a neat, toughened, heat stabilized polyphthalamide (PPA) resin that offers superior retention of properties after humid thermal aging; high impact at low temperature and bet.. |
|||
Flexural Modulus | 1.72 GPa | 249 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics XYLEX X8303CL PC+POLYESTER (Asia Pacific) PC+ POLYESTER, Transparent, Low processing Temperature, High flow with excellent impact, UV stabilized, OQ quality. For In Mold Decoration /Labeling. |
|||
Flexural Modulus | 1.72 GPa | 249 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics XYLEX X8303CL PC+POLYESTER (Europe-Africa-Middle East) PC+ POLYESTER, Transparent, Low processing Temperature, High flow with excellent impact, UV stabilized, OQ quality. For In Mold Decoration /Labeling. |
|||
Flexural Modulus | 1.72 GPa | 249 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® GC-0770 H ABS/PET, Unreinforced Recycled Eco-friendly Post-Consumer recycled PET.Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 1.72 GPa | 249 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® SP-0170 ABS, Unreinforced Extrusion Grade Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 1.72 GPa | 249 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® SP-0170 ABS, Unreinforced Extrusion Grade Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 1.72 GPa | 249 ksi | ASTM D790 |
Samyang Triloy® 120H PC/ABS alloy Characteristics:Impact resistantChemical resistantDimensional stabilityProcessabilityGood flowApplications:Automotive bumperAutomotive outdoor handleAll information provided by Samyang |
|||
Flexural Modulus | 1.72 GPa | 249 ksi | ASTM D790 |
Covestro Bayflex® 190 Polyurethane Elastomeric RIM, 20% Mineral Filled, MDI-based 2-Component Liquid System 0.150 in. thickness. Calcium Silicate filled. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was se.. |
|||
Flexural Modulus | 1.72 GPa | 249 ksi | ASTM D790 |
Braskem CP 405 XP Injection Molding Polypropylene Applications: Caps for soft drinks. Information provided by Braskem |
|||
Flexural Modulus | 1.72 GPa | 249 ksi | |
Plastcom SLOVALEN PH 61 GB 30 PP, 30% glass beads, mod. of mech. prop. FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 30% glass beads, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP... |
|||
Flexural Modulus | 1.72 GPa | 249 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON QD000I PA 6/10 LNP* STAT-KON* QD000I is a compound based on Nylon 6/10 resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact. |
|||
Flexural Modulus | 1.72 GPa | 249 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON QD000I PA 6/10 (Asia Pacific) LNP STAT-KON* QD000I is a compound based on Nylon 6/10 resin containing Carbon Powder. Added features of this material include: Electrically Conductive. |