Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 17.0 GPa | 2470 ksi | ISO 178 |
PolyOne OnForce™ LFT NN-60LGF/000 HS Natural Polyamide 66 (Nylon 66) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Flexural Modulus | 17.0 GPa | 2470 ksi | 1.3 mm/min; ASTM D790 |
PolyOne Edgetek® PC-30CF/000 BLACK Polycarbonate (PC) Information provided by PolyOne |
|||
Flexural Modulus | 17.0 GPa | 2470 ksi | ISO 178 |
Victrex® WG101™ Polyaryletherketone Product Description: High performance thermoplastic material, PolyArylEtherKetone (PAEK), semi crystalline, black, granules for injection moulding, easy flow with wear additivesWG101 does not contai.. |
|||
Flexural Modulus | 17.0 GPa | 2470 ksi | ISO 178 |
Victrex® WG102™ Polyaryletherketone Product Description: High performance thermoplastic material, PolyArylEtherKetone (PAEK), semi crystalline, granules for injection moulding, standard flow, FDA food contact compliantWG102 does not c.. |
|||
Flexural Modulus | 17.0 GPa | 2470 ksi | ISO 178 |
Solvay Specialty Polymers Ixef® 2011 Polyarylamide (PARA), 42% Mineral Filler
(discontinued **) Ixef 2011 is a general purpose, 42% mineral reinforcedpolyarylamide which exhibits high strength and stiffness, low warpage, and outstanding surface gloss.- Black: Ixef 2011/9000- Custom ColorableFe.. |
|||
Flexural Modulus | 17.0 GPa | 2470 ksi | |
Cookson Group Plaskon® 1002 Conventional Encapsulant
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.A low cost, low stress, conventional molding compound recommended for high volume commodity-type packages that house simple linea.. |
|||
Flexural Modulus | 17.0 GPa | 2470 ksi | ISO 178 |
Hexion Bakelite™ PF 4109 Phenolic Formaldehyde Resin, Improved Electrical Properties, Ammonia Free, Resistant to High Temperatures, Low Shrinkage, High Arc Resistance, UL Listed, Acetic Acid Free Phenolic molding compound, inorganically filled, glass fiber reinforced, ammonia and acetic acid free, electrically high grade, high temperature stability, low shrinkage, high mechanical strength, U.. |
|||
Flexural Modulus | 17.0 GPa | 2470 ksi | |
Lehmann & Voss LUVOCOM® 1501/CF/30-1 Polysulfone, with carbon fiber Applications: Automotive industry, office machinery, medical- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Chemical and hydrolysis resistance parts, non.. |
|||
Flexural Modulus | 17.0 GPa | 2470 ksi | |
Lehmann & Voss LUVOCOM® 1-7532 Polyamide 66, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Flexural Modulus | 17.0 GPa | 2470 ksi | |
Lehmann & Voss LUVOCOM® 19-7900 Polyamide 46, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Flexural Modulus | 17.0 GPa | 2470 ksi | |
Lehmann & Voss LUVOCOM® TPI-8257 Thermoplastic polyimide, with carbon fiber Applications: Automotive industry, textile machinery, apparatus- and precision engineering medical- and electrical enineering, aircraft- and aerospace industry.High-strength and high-stiff parts; lo.. |
|||
Flexural Modulus | 17.0 GPa | 2470 ksi | ASTM D790 |
Mitsui Arlen™ A350 50% Glass Fiber-Reinforced Modified Nylon 6T (DAM) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
Flexural Modulus | 17.0 GPa | 2470 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP JCL36 PES (Europe-Africa-Middle East) LNP* LUBRICOMP* JCL36 is a compound based on Polyethersulfone resin containing Carbon Fiber, PTFE. Added features include : Internally Lubricated, Electrically Conductive. |
|||
Flexural Modulus | 17.0 GPa | 2470 ksi | ISO 178 |
Solvay Specialty Polymers Ixef® 1025 Polyarylamide (PARA), 50% Glass Fiber Ixef® 1025 is a 50% glass-fiber reinforced, UV stabilized polyarylamide which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Features: Good Ch.. |
|||
Flexural Modulus | 17.0 GPa | 2470 ksi | ISO 178 |
Solvay Specialty Polymers Kalix® 2855 Polyamide, High Performance (HPPA), Glass Fiber Kalix® 2855 is a 27% bio-sourced, PA 6,10-based compound with 55% by weight glass fiber reinforcement. This material is formulated to provide maximum strength, stiffness, impact resistance, and p.. |
|||
Flexural Modulus | 17.0 GPa | 2470 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP LC006 PEEK (Europe-Africa-Middle East) LNP* THERMOCOMP* LC006 is a compound based on Polyetheretherketone containing Carbon Fiber. Added features include: Electrically Conductive. |
|||
Flexural Modulus | 17.0 GPa | 2470 ksi | ISO 178 |
SABIC Innovative Plastics LNP Thermocomp WC006 Polyester, TP LNP* Thermocomp* WC006 is a compound based on Polyester, TP resin containing Carbon Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 17.0 GPa | 2470 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP WC006 Polyester, TP (Asia Pacific) LNP* Thermocomp* WC006 is a compound based on Polyester, TP resin containing Carbon Fiber. |
|||
Flexural Modulus | 17.0 GPa | 2470 ksi | ASTM D790 |
Sumitomo Bakelite North America E 8398 Hardware Grade Epoxy Fiberglass and mineral reinforced epoxy molding compound with excellent dimensional stability, good electrical insulation properties, and good strength.Information provided by Vyncolit, a Sumitomo B.. |
|||
Flexural Modulus | 17.0 GPa | 2470 ksi | ISO 178 |
Vyncolit Neopreg Kinel® SK80 L8G Glass Fiber Reinforced Molding Compound Epoxy based molding compound long glass fiber reinforced with excellent long term property retention over a wide temperature range and climate conditions. It is particularly suited for over mold.. |
|||
Flexural Modulus | 17.0 GPa | 2470 ksi | ISO 178 |
Vyncolit X640 Resole Phenolic Glass fiber filled phenolic molding compound with excellent mechanical and thermal properties.USES: Information provided by Vyncolit, a Sumitomo Bak Group |
|||
Flexural Modulus | 17.0 - 22.0 GPa | 2470 - 3190 ksi | Longitudinal |
Goodfellow Polyaramid/Vinylester Composite Tube or Rod Information provided by Goodfellow. |
|||
Flexural Modulus | 17.0 GPa | 2470 ksi | dry; ISO 178 |
DSM Stanyl® OCD2300 BLK PA46-GF50 50% Glass Reinforced, Heat Stabilized |
|||
Flexural Modulus | 17.0 GPa | 2470 ksi | transverse; ISO 178 |
Bond Laminates TEPEX® dynalite 104-RG600(x)/47% Roving Glass – PP Consolidated Composite Laminate Within the TEPEX® composite laminate, PP is a resin known for its good hardness, stiffness, abrasion resistance and chemical resistance.Typical application environments are within automotive applic.. |
|||
Flexural Modulus | 17.0 GPa | 2470 ksi | 2 [mm/min]; ISO 178 |
Akro-Plastic Akromid® B3 GF 50 RM-M (3146) PA 6 Dry, 50% Glass Filled In all, the construction relevant features show that the significantly reduced moisture absorption of AKROMID B3 GF 30 RM leads to increasing rigidities and strengths as already expected. Neverthele.. |
|||
Flexural Modulus | 17.0 GPa | 2470 ksi | ISO 178 |
Vyncolit Neopreg Kinel® SK60 L8F Glass Fiber Reinforced Molding Compound Medium flow, epoxy based molding compound long glass fiber reinforced with excellent long term property retention over a wide temperature range and climate conditions. It is particularly suited f.. |
|||
Flexural Modulus | 17.0 GPa | 2470 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON REF42 PA 66 (Asia Pacific) LNP* Stat-kon* REF42 is a compound based on Nylon 66 resin containing Glass Fiber, Carbon Fiber. |
|||
Flexural Modulus | 17.0 GPa | 2470 ksi | ASTM D790 |
Resinoid 7051 SS Phenolic Molding, Glass Reinforced Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance |