Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.68 GPa @Temperature 23.0 °C |
243 ksi @Temperature 73.4 °F |
ASTM D790A |
Ineos H11G-00 Polypropylene Homopolymer This is a barefoot homopolymer designed for fiber applications.ApplicationsStaple FiberOriented YarnBenefitsConsistent processabilityInformation provided by Ineos Olefins & Polymers USA |
|||
Flexural Modulus | 1.67 - 82.7 GPa | 243 - 12000 ksi | Average value: 8.92 GPa Grade Count:42 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified". Each property range of values reported.. |