Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 16.7 GPa | 2420 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP PF00C PA 6 (Europe-Africa-Middle East) LNP* THERMOCOMP* PF00C is a compound based on PA6 resin containing Glass Fiber. |
|||
Flexural Modulus | 16.7 GPa | 2420 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP PF00CS PA 6 (Europe-Africa-Middle East) LNP* THERMOCOMP* PF00CS is a compound based on PA6 resin containing Glass Fiber. |
|||
Flexural Modulus | 16.7 GPa | 2420 ksi | ASTM D790 |
E-Polymers TEKAMID® TA250G60 60% Glass Fiber Reinforced, High Modulus PA66 Resin Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.T-series: Impact modified,.. |