Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.615 GPa | 234.3 ksi | ASTM D790 |
KKPC Kuhmo HI 425EP Extrusion Molding HIPS Common Uses: Refrigerator inner liners, door liners, disposable cups, food packaging sheet, wrapping films, trays, washing machinesHIPS is a functional resin made by copolymerization of styrene mono.. |
|||
Flexural Modulus | 1.615 GPa | 234.3 ksi | ASTM D790 |
KKPC Kuhmo HI 425TVD High Flow/High Heat Resistant HIPS Key features: High-impact-fluidity. Common Uses: TV cover, computer case.HIPS is a functional resin made by copolymerization of styrene monomer and PBR. It shows excellent balance between impact-res.. |
|||
Flexural Modulus | 1.615 GPa | 234.3 ksi | ASTM D790 |
KKPC Kuhmo HI 425TVG High Flow/High Heat Resistant HIPS Key features: High-impact, High-fluidity Common Uses: TV cover (gas injection).HIPS is a functional resin made by copolymerization of styrene monomer and PBR. It shows excellent balance between im.. |
|||
Flexural Modulus | 1.615 GPa | 234.3 ksi | ASTM D790 |
KKPC Kuhmo HI 425TVL High Flow/High Heat Resistant HIPS Key features: Super high-fluidity. Common Uses: TV cover (Fine TV), Drawers.HIPS is a functional resin made by copolymerization of styrene monomer and PBR. It shows excellent balance between impact-.. |