Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.60 GPa | 232 ksi | ASTM D790 |
NYCOA 1595 HS Impact Modified, Medium Viscosity Nylon 6 Resin NYCOA 1595 HS is a medium viscosity Nylon 6 resin, which offers superior flexibility and toughness in both molding and extrusion applications. Its high melt viscosity and strength provides excellent.. |
|||
Flexural Modulus | 1.60 GPa | 232 ksi | STN EN ISO 178 |
Plastcom SLOVALEN PC 51 C 40 LS/1M Polypropylene reinforced with mineral filler, UV stabilized Modified copolymer PP for injection molding with the content of 40% mineral filler, UV stabilized. Product meets glow wire test at 750°C. Delivered in full RAL color scale.Information Provided by P.. |
|||
Flexural Modulus | 1.60 GPa | 232 ksi | ISO 178 |
Polyplastic Armlen® PP-2FR Polypropylene, Flame Retardant Flame retardant, RoHS compliantInformation provided by PolyPlastic Group. |
|||
Flexural Modulus | 1.60 GPa @Temperature 23.0 °C |
232 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYfill PPC K5025 PP, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Modulus | 1.60 GPa | 232 ksi | ASTM D790 |
Shell Carilon® D26CX100 Polyketone, Advanced Extrusion Grade
(discontinued **) Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON Polymer D26CX100 is an extrusion grade with mechanical properties that classify it as an engineering thermo.. |
|||
Flexural Modulus | 1.60 GPa | 232 ksi | ISO 178 |
Grupo Repol Dinalon® B1S25 DI PA6 Dry Impact Mechanical properties for Dry As Molded samplesInformation provided by Grupo Repol |
|||
Flexural Modulus | 1.60 GPa | 232 ksi | 1% Secant; ASTM D790 |
IRPC Polimaxx Polene 1202J Polypropylene Homopolymer CHARACTERISTICS: GOOD STIFFNESS, GOOD EXTRUDABILITY, HIGH IMPACTAPPLICATIONS: MONOFILAMENT/YARN/SHEET EXTRUSION AND INJECTION MOLDING COARSE TEXTILE FOR JUMBO BAGS, ROPES, STRAWS, SHEETS, INDUSTRIAL.. |
|||
Flexural Modulus | 1.60 GPa | 232 ksi | ISO 178 |
LyondellBasell Hostacomâ„¢ CB267 Thermoplastic Polyolefin Elastomer Description: Hostacomâ„¢ CB267 medium melt flow, 1,600 MPa flexural modulus thermoplastic elastomeric olefin (TEO) resin has an excellent balance of scratch and mar resistance, rigidity and impac.. |
|||
Flexural Modulus | 1.60 GPa | 232 ksi | ISO 178 |
SABIC Innovative Plastics LNP Stat-loy A3000Z ABS (Asia Pacific) LNP* Stat-loy* A3000Z is a compound based on Acrylonitrile Butadiene Styrene resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for t.. |
|||
Flexural Modulus | 1.60 GPa | 232 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-LOY KX01002 Acetal Copolymer (Europe-Africa-Middle East) LNP* Stat-Loy* KX01002 is a compound based on Acetal Copolymer resin containing Antistat. Added features include: Permanent Anti-Static. |
|||
Flexural Modulus | 1.60 GPa | 232 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics XYLEX X8210 PC+POLYESTER PC+POLYESTER alloy. Unreinforced, transparent, impact modified for low temperature ductility |
|||
Flexural Modulus | 1.60 GPa | 232 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics XYLEX X8210 PC+POLYESTER (Europe-Africa-Middle East) PC+POLYESTER alloy. Unreinforced, transparent, impact modified for low temperature ductility |
|||
Flexural Modulus | 1.60 GPa | 232 ksi | ASTM D790 |
Teknor Apex Sinpolene TPP2010 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Talc Filler, 10% Filler by Weight Uses: Appliance Components; Automotive Applications; Housings Forms: Pellets Process.. |
|||
Flexural Modulus | 1.60 GPa | 232 ksi | ASTM-D790 |
Polyram PlusTek PB891 Nylon 6, Impact Modified Impact modified polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Flexural Modulus | 1.60 GPa | 232 ksi | ISO 527-2 |
Total PPH 5042 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 5042 is homopolymer.ApplicationATOFINA Polypropylene PPH 5042 has been specially designed for extrusion-thermoforming, where it gives improved rigidity and impact resistanc.. |
|||
Flexural Modulus | 1.60 GPa | 232 ksi | ASTM D790 |
Goodfellow TPX® RT31XB Injection Molding Grade Polymethylpentene This grade is highly recommended for injection molding; also for film and fiber extrusion.TPX® is semi-crystalline, transparent, very light and - for a polyolefin - expensive. It has good release c.. |
|||
Flexural Modulus | 1.60 GPa | 232 ksi | ISO 178 |
Total PSI 8350 High Impact Polystyrene 8350 is a very high impact polystyrene for extrusion. This grade has an improved environmental stress crack resistance in comparison with standard high impact grades. It is proposed for the produc.. |
|||
Flexural Modulus | 1.60 GPa | 232 ksi | ASTM D790 |
A. Schulman POLYFORT™ FXP 3000-3120 Glass Sphere Filled Copolymer Polypropylene DescriptionPolyfort® FXP 3000-3120 is a 30% glass sphere filled copolymer polypropylene compound.Information provided by A. Schulman. |
|||
Flexural Modulus | 1.60 GPa | 232 ksi | cond; ISO 178 |
DSM Novamid® 3010N 5-SL4-3X NAT PA66 FR Low Viscosity, Molding Release, 30% Glass Reinforced |
|||
Flexural Modulus | 1.60 GPa | 232 ksi | 2 mm/min; ISO 178 |
Chi Mei Polyrex® PH-60 Polystyrene - High Impact Medium impact |
|||
Flexural Modulus | 1.60 GPa | 232 ksi | ASTM D790 |
Braskem H 117 Injection Molding Polypropylene Description: H 117 is a ultra-high melt flow rate homopolymer. This product is suitable to high productivity on thin-walled parts. H 117 features an excellent stiffness, thermal resistance, low warp.. |
|||
Flexural Modulus | 1.60 - 6.40 GPa @Temperature -40.0 - 80.0 °C |
232 - 928 ksi @Temperature -40.0 - 176 °F |
Average value: 4.28 GPa Grade Count:1 |
Overview of materials for Nylon 66, 20% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are inclu.. |
|||
Flexural Modulus | 1.60 GPa | 232 ksi | ASTM D790 |
Shell Carilon® D26HM100 Polyketone, General-Purpose Injection Molding Grade
(discontinued **) Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON Polymer D26HM100 is a general-purpose injection molding grade with mechanical properties which classify it .. |
|||
Flexural Modulus | 1.60 GPa | 232 ksi | ASTM D790 |
Adell RZ-18 Copolymer Polypropylene, 40% Calcium Carbonate Filled Data provided by Adell Plastics, Inc. |
|||
Flexural Modulus | 1.60 GPa | 232 ksi | ASTM D790 |
A. Schulman POLYFORT™ FXP 3000-3120 Glass Sphere Filled Copolymer Polypropylene DescriptionPolyfort® FXP 3000-3120 is a 30% glass sphere filled copolymer polypropylene compound.Information provided by A. Schulman. |
|||
Flexural Modulus | 1.60 GPa | 232 ksi | ISO 178 |
Unipetrol PP MONSTEN® GB 003 Polypropylene Homopolymer Applications include injection molding, tapes, and thermoforming. Basic stabilization. Homopolymer.Information provided by Unipetrol RPA |
|||
Flexural Modulus | 1.60 GPa | 232 ksi | ASTM D790 |
A. Schulman POLYFORT™ FXP 3000-3120 Glass Sphere Filled Copolymer Polypropylene DescriptionPolyfort® FXP 3000-3120 is a 30% glass sphere filled copolymer polypropylene compound.Information provided by A. Schulman. |
|||
Flexural Modulus | 1.60 GPa | 232 ksi | 2 mm/min; ISO 178 |
Sax Polymers SAXALEN PPH329B20 Polypropylene Homopolymer, 20% Glass Filled SAXALEN PPH329B20 is a 20% glass beads filled Polypropylene - Homopolymer intended for injection molding. Low shrinkage, low warpage gradeInformation provided by SAX Polymers |