Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 15.9 GPa | 2310 ksi | ASTM D790 |
PolyOne Gravi-Tech™ GRV-NY-112-W-NAT Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Flexural Modulus | 15.9 GPa @Temperature 23.0 °C |
2310 ksi @Temperature 73.4 °F |
ISO 178 |
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent creep .. |
|||
Flexural Modulus | 15.9 GPa | 2310 ksi | (50.8 mm Span) 1mm/min; ASTM D790 |
LNP ULTEM® EXCP0096 Polyetherimide, 30% Carbon Fiber Reinforcement, 10% PTFE Lubricant
(discontinued **) Features: Lubricated, Electrically Conductive, Good Wear Resistance, High Heat ResistanceForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This dat.. |
|||
Flexural Modulus | 15.9 GPa @Temperature 23.0 °C |
2310 ksi @Temperature 73.4 °F |
ISO 178 |
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA), 45% Glass Fiber (Dry) Amodel® A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent cr.. |
|||
Flexural Modulus | 15.9 GPa | 2310 ksi | ISO 178 |
Solvay Specialty Polymers Kalix® 9950 Polyamide, High Performance (HPPA), 50% Glass Fiber Kalix® 9950 is a 50% glass-fiber reinforced high-performance polyamide. It is hot-water moldable and intended for use in components requiring superior mechanical properties and excellent surface .. |
|||
Flexural Modulus | 15.9 GPa | 2310 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP EC006 PEI (Europe-Africa-Middle East) LNP* THERMOCOMP* EC006 is a compound based on Polyetherimide resin containing Carbon Fiber. Added features include: Electrically Conductive. |
|||
Flexural Modulus | 15.9 GPa | 2310 ksi | ASTM D790 |
Sumitomo Bakelite North America Epiall® 1908B-1 Short Glass Fiber Reinforced Epoxy Epiall 1908B-1 is a short fiberglass reinforced epoxy molding compound, with excellent dimensional stability, good strength properties and good electrical insulation properties.Information provided .. |
|||
Flexural Modulus | 15.9 GPa | 2310 ksi | ASTM D790 |
Sumitomo Bakelite North America Epiall® 2061B-1 Mineral and Glass Filled Electrical Encapsulation Grade Epoxy Epiall 2061B-1 is a fiberglass and mineral reinforced epoxy molding compound, with excellent dimensional stability, good electrical insulation properties, and good strength.Information provided by S.. |
|||
Flexural Modulus | 15.9 GPa | 2310 ksi | ASTM D790 |
Plenco 7556 Phenolic, Briquette, Transfer Molded PLENCO 07556 is a glass fiber reinforced novolac phenolic molding compound, with good physical strengths and heat resistance along with excellent dimensional stability. UL recognized under component.. |
|||
Flexural Modulus | 15.9 GPa | 2310 ksi | ASTM D790 |
Sumitomo Bakelite North America RX® 647 Fiberglass Reinforced Phenolic RX 643 is a fiberglass reinforced, ammonia-free, phenolic resole compound, with good dimensional stability and good strength at elevated temperatures. Meets ASTM D-5948 Type GPI-10. RX 647 is a fibe.. |
|||
Flexural Modulus | 15.9 GPa | 2310 ksi | ASTM D790 |
Sumitomo Bakelite North America RX® 853G Fiberglass Reinforced Phenolic Novolac RX 853G is a fiberglass reinforced phenolic novolac compound, featuring dimensional stability, moderate impact resistance, and good strength and modulus.Information supplied by Sumitomo Bak North Am.. |
|||
Flexural Modulus | 15.9 GPa | 2310 ksi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 716 PPS, Carbon Fiber Reinforced Data provided by the manufacturer, ComAlloy International Company.20% Carbon Fiber Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |