Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 15.9 GPa @Temperature 23.9 °C |
2300 ksi @Temperature 75.0 °F |
Dry; 325°F Autoclave; ASTM D790 |
Park Electrochemical Nelcote® F-557 Phenolic Prepreg, Aerospace Silica Fabric Reinforced Nelcote® F-557 is a high purity silica filler phonic resin coated on Commercial or Aerospace grade silica fabric. F-557 is used in the manufacture of intermediate temperature ablative rocket nozzle.. |
|||
Flexural Modulus | 15.9 GPa | 2300 ksi | |
MTI ThermoStran® TPU-60G Long Glass Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |
|||
Flexural Modulus | 15.9 GPa | 2300 ksi | ASTM D790 |
Techmer ES Electrafil® J-1200/CF/40 NAT ABS |
|||
Flexural Modulus | 15.9 GPa | 2300 ksi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF50 HS L BK 50% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearanc.. |
|||
Flexural Modulus | 15.9 GPa | 2300 ksi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF50 L BK 50% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: LubricantFeatures: Lubricated Appearance: BlackInformation provided by TP Comp.. |
|||
Flexural Modulus | 15.9 GPa | 2300 ksi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF50 L UV 50% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Lubricant and UV StabilizerFeatures: Lubricated and Good UV ResistanceInformat.. |
|||
Flexural Modulus | 15.9 GPa | 2300 ksi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF50 X BK 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAppearance: BlackTPCI# 6560101Information provided by TP Composites, Inc. |
|||
Flexural Modulus | 15.9 GPa | 2300 ksi | ASTM D790 |
Techmer ES HiFill® PEEK CF30 HF 30% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 30% Filler by WeightFeatures: High FlowInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 15.9 GPa | 2300 ksi | ASTM D790 |
Techmer ES Luriblend® PPA CF30 TL15 30% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAdditive: PTFE Lubricant(15%)Features: Lubricated, Good Wear Resistance, High Heat Resistance and Low.. |
|||
Flexural Modulus | 15.9 GPa | 2300 ksi | ASTM D790 |
Techmer ES Electrablend® PA6 CF30 30% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 30% Filler by WeightFeatures: Conductive Appearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 15.9 GPa | 2300 ksi | ASTM D790 |
Techmer ES HiFill® PPS/F GF10 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightAppearance: Natural ColorInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 15.9 GPa | 2300 ksi | ASTM D790 |
Clariant Renol PPSS0007 Polyphenylene Sulfide, Glass Fiber and Mineral Filled Data provided by Clariant Masterbatches |