Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 2280 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 15.7 GPa

@Thickness 3.20 mm
2280 ksi

@Thickness 0.126 in
1.3mm/min; ASTM D790
LG Chemical LUMID HM2604AW PA6+GF60%
Feature: Injection Molding, PA6+GF60%Application: Bath liftInformation provided by LG Chemical
Flexural Modulus 15.7 GPa
2280 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP OE004A PPS - BRANCHED (Europe-Africa-Middle East)
LNP* STATKON* OE004A is a compound based on PPS (branched) resin containing Carbon Fiber. Added features include: Electrically Conductive. (only Black is UL listed)
Flexural Modulus 15.7 GPa
2280 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP STAT-KON OE004A PPS - BRANCHED (Europe-Africa-Middle East)
LNP* STATKON* OE004A is a compound based on PPS (branched) resin containing Carbon Fiber. Added features include: Electrically Conductive.
Flexural Modulus 15.7 GPa
2280 ksi
Phenolic 40%, Carbon fabric 60%
Phenolic - Monsanto "SC 1008". Carbon fabric - "CCA-1"
Copyright © lookpolymers.com All Rights Reserved