Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.52 GPa | 220 ksi | Tangent; ASTM D790 |
RheTech Products P100-01 Polypropylene Homopolymer, Black Applications: Wire harnessesTrim componentsUnderhood applicationsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 1.52 GPa | 220 ksi | 0.05 in/min; 1% secant; Procedure A; ASTM D790 |
Phillips 66 COPYLENE® CM040LN Polypropylene, Impact Copolymer, Thermoforming COPYLENE™ CM040LN is an impact copolymer specially designed for excellent processing in thermoforming applications and is formulated with antistat and nucleation. Applications: Thermoforming, Injec.. |
|||
Flexural Modulus | 1.52 GPa | 220 ksi | ASTM D790 |
Multibase Multi-Pro® 2510 XG Polypropylene Mineral Filled, 25% by weight.Features:Gloss, HighForms:PelletsProcessing Methods:Injection MoldingUses:AppliancesFurnitureInformation provided by Multibase |
|||
Flexural Modulus | 1.52 GPa | 220 ksi | ASTM D790 |
PolyOne Maxxam™ DP-9156-5-8000 Polypropylene Copolymer (PP Copolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Flexural Modulus | 1.52 GPa | 220 ksi | ASTM D790 |
PolyMirae Moplen HP500G Sheet and Thermoforming Grade Polypropylene Moplen HP500G is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP500G is a homopolymer particularly suitable for sheet, thermofor.. |
|||
Flexural Modulus | 1.52 GPa | 220 ksi | ASTM D790 |
LyondellBasell Petrothene® LM600500 High Density Polyethylene ApplicationsPETROTHENE LM 6005-00 resin is especially designed for water, milk, and juice bottles. It exhibits excellent rigidity and good processability.Regulatory StatusLM 6005-00 meets the requi.. |
|||
Flexural Modulus | 1.52 GPa | 220 ksi | 1% Secant; ASTM D790 |
Flint Hills P4C5N-046 Homopolymer Polypropylene Homopolymer, UL certified, and FDA compliant.Features: Nucleated and controlled rheology.Applications: Injection molding: general purpose.Former Huntsman polypropylene products are now produced by F.. |
|||
Flexural Modulus | 1.52 GPa | 220 ksi | Secant @ 1% strain; ASTM D790 |
Ineos H00G-00 Polypropylene Homopolymer A polypropylene homopolymer produced by Ineos utilizing catalyst technology. This material meets the Food and Drug Administration requirements of 21CFR 177.1520. Homopolymer H00G-00 meets certain .. |
|||
Flexural Modulus | 1.52 GPa @Temperature 23.0 °C |
220 ksi @Temperature 73.4 °F |
ASTM D790A |
Ineos H20Z-03 Polypropylene Homopolymer This is a homopolymer containing nucleation and antistatic. It is designed for injection molding and meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520... |
|||
Flexural Modulus | 1.52 GPa | 220 ksi | 5 mm/min; ISO 178 |
Gromax ATE90-FN01N1 Nylon 6 (Dry) Information provided by Gromax Enterprises Corp. |
|||
Flexural Modulus | 1.52 GPa | 220 ksi | secant; ASTM D790 |
Spartech PE4325 Reinforced High Density Polyethylene Compound Spartech Polycom's filled high molecular weight, high density polyethylenes are specifically designed for blow molding and sheet extrusion /thermoforming of structural parts. These materials offer a.. |
|||
Flexural Modulus | 1.52 GPa | 220 ksi | ASTM D790 |
A. Schulman PP 3468-01 Polypropylene Homopolymer For High Speed Extrusion DescriptionPolypropylene PP 3468-01 is a specially designed homopolymer for high speed extrusion applications. ApplicationTypical applications of PP 3468-01 include profile extrusions, strapping, r.. |
|||
Flexural Modulus | 1.52 GPa | 220 ksi | ASTM D790 |
A. Schulman PP 3468-01 Polypropylene Homopolymer For High Speed Extrusion DescriptionPolypropylene PP 3468-01 is a specially designed homopolymer for high speed extrusion applications. ApplicationTypical applications of PP 3468-01 include profile extrusions, strapping, r.. |
|||
Flexural Modulus | 1.52 GPa | 220 ksi | Tangent; ASTM D790 |
Washington Penn Medium Impact Copolymer 10% Talc Filled Talc-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug packaging requi.. |
|||
Flexural Modulus | 1.52 GPa | 220 ksi | ASTM D790 |
A. Schulman PP 3468-01 Polypropylene Homopolymer For High Speed Extrusion DescriptionPolypropylene PP 3468-01 is a specially designed homopolymer for high speed extrusion applications. ApplicationTypical applications of PP 3468-01 include profile extrusions, strapping, r.. |
|||
Flexural Modulus | 1.52 GPa | 220 ksi | |
Astaras ANVILOY® 1150 Tungsten Based High Temp Alloy Anviloy® 1150 is a tungsten-based material that was developed primarily for die-casting, aluminum permanent mold, and difficult extrusions. It is produced by a high temperature powder metallurgy pr.. |
|||
Flexural Modulus | 1.52 GPa | 220 ksi | ASTM D790 |
Clariant Renol PA1SP0004 Nylon 66, High Impact Modified, ESD Data provided by Clariant Masterbatches |
|||
Flexural Modulus | 1.52 GPa | 220 ksi | |
CMW® ELKONITE® TC53 Heat Treatable Tungsten Carbide Copper material For electroforging and electrical upsetting dies.Information provided by CMW Inc. |
|||
Flexural Modulus | 1.52 - 2.07 GPa | 220 - 300 ksi | ASTM D790 |
3D Systems Accura® Xtreme White 200 Plastic Ultra tough white plastic to replace CNC Machined polypropylene and ABS articles FeaturesExceptionally tough and durableUsed for challenging functional assembliesUsed for snap fit assembl.. |
|||
Flexural Modulus | 1.52 GPa | 220 ksi | ASTM D790 |
Asahi Kasei Thermylene® P-20TC-0736 20% Talc Filled, Heat Stabilized Information provided by Asahi Thermofil |
|||
Flexural Modulus | 1.52 GPa | 220 ksi | 0.05 in/min; 1% secant; Procedure A; ASTM D790 |
Phillips 66 COPYLENE® CH008 Polypropylene, Homopolymer, Netting COPYLENE™ CH008 is a fractional melt flow polypropylene homopolymer resin available in pellet form. Applications: Raffia/Tapes/Strapping; Anti-Corrosion Coating; Geotextile & Agriculture; Nets. Rep.. |
|||
Flexural Modulus | 1.52 GPa | 220 ksi | ASTM D790 |
Quadrant EPP Semitron® ESd 225, Extruded, Static Dissipative Acetal (ASTM Product Data Sheet) |
|||
Flexural Modulus | 1.52 GPa | 220 ksi | ASTM D790A |
Ineos H35G-01 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: General purposeTypical applications: Rigid packaging, Consumer products, CompoundingComplies with FDA specification, Title 21, CFR 177.1520... |
|||
Flexural Modulus | 1.52 GPa | 220 ksi | 0.05 in/min, 1% secant; ASTM D-790A |
Braskem D130C Homopolymer Polypropylene Description: High BulkApplications: Suggested Uses Include Fine Denier Staple Fiber, High Speed Fiber SpinningThis resin meets the requirements for olefin polymers as defined in 21 CFR, section 177... |