Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 15.16 GPa | 2199 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Stat-kon EE006EM PEI LNP* Stat-kon* EE006EM is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding.This data was supplied by .. |
|||
Flexural Modulus | 15.16 GPa | 2199 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Stat-kon EE006EM PEI (Asia Pacific) LNP* Stat-kon* EE006EM is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding.This data was supplied by .. |
|||
Flexural Modulus | 15.16 GPa | 2199 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON REP349 PA 66 LNP* STAT-KON* REP349 is a compound based on Nylon 66 resin containing 15% PTFE/Silicone, 20% Carbon Fiber. Added features of this material include: Electrically Conductive, Wear Resistant. |
|||
Flexural Modulus | 15.16 GPa | 2199 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON REP349 PA 66 (Asia Pacific) LNP* Stat-kon* REP349 is a compound based on Nylon 66 resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubricated. |
|||
Flexural Modulus | 15.16 GPa | 2199 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp WC006 Polyester, TP LNP* Thermocomp* WC006 is a compound based on Polyester, TP resin containing Carbon Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 15.16 GPa | 2199 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP WC006 Polyester, TP (Asia Pacific) LNP* Thermocomp* WC006 is a compound based on Polyester, TP resin containing Carbon Fiber. |
|||
Flexural Modulus | 15.16 GPa | 2199 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP WC006 PBT LNP* THERMOCOMP* WC006 is a compound based on PBT resin containing 30% Carbon Fiber. Added feature of this grade is: Electrically Conductive. |