Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.150 GPa | 21.8 ksi | ISO 178 |
Polimeri Europa Flexirene® MS 20 A Linear Low Density Polyethylene Flexirene MS 20 A is a linear low density polyethylene (LLDPE), with antioxidants, suitable for injection molding application.Parts made with Flexirene MS 20 A are characterized by optimum low tempe.. |
|||
Flexural Modulus | 0.150 GPa | 21.8 ksi | ISO 178 |
Polimeri Europa Flexirene® MS 20 U Linear Low Density Polyethylene Flexirene MS 20 U is a linear low density polyethylene (LLDPE), with antioxidants, suitable for injection molding application.Parts made with Flexirene MS 20 U are characterized by optimum low tempe.. |
|||
Flexural Modulus | 0.150 GPa | 21.8 ksi | ISO 178 |
Polimeri Europa Flexirene® MS 26 A Linear Low Density Polyethylene Flexirene MS 26 A is a linear low density polyethylene (LLDPE), with antioxidants, suitable for injection molding application.Parts made with Flexirene MS 26 A are characterized by optimum low tempe.. |
|||
Flexural Modulus | 0.150 GPa | 21.8 ksi | ASTM D790 |
Rotuba H4 Cellulose Acetate Property values at 50% RH.Data provided by the manufacturer. |
|||
Flexural Modulus | 0.150 GPa | 21.8 ksi | ASTM D790 |
ExxonMobil Iotek® 7610 Zinc Ionomer
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A low melt index zinc ionomer made from an ethylene acrylic acid base polymer. It is designed to have high durability, resilience and impact streng.. |
|||
Flexural Modulus | 0.150 GPa | 21.8 ksi | 12.5 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL WCD861A PPE-TPE Flexible, migration-improved, halogen free extrusion grade intended for evaluation in applications such as wire insulation and cable jacket. Flame performance capable of meeting UL VW1 requirements.. |
|||
Flexural Modulus | 0.150 GPa | 21.8 ksi | 12.5 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL WCD861A PPE-TPE (Asia Pacific) Flexible, migration-improved, halogen free extrusion grade intended for evaluation in applications such as wire insulation and cable jacket. Flame performance capable of meeting UL VW1 requirements.. |
|||
Flexural Modulus | 0.150 GPa | 21.8 ksi | 12.5 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL WCD861A PPE-TPE (Europe-Africa-Middle East) Flexible, migration-improved, halogen free extrusion grade intended for evaluation in applications such as wire insulation and cable jacket. Flame performance capable of meeting UL VW1 requirements.. |
|||
Flexural Modulus | 0.150 GPa | 21.8 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DEL22P PC LNP STAT-KON* DEL22P is a compound based on Polycarbonate resin containing 10% Carbon Fiber, 10% PTFE. Added features of this material include: Electrically Conductive. Exceptional Processing, Wear.. |
|||
Flexural Modulus | 0.150 GPa | 21.8 ksi | 12.5 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL WCD851 PPE-TPE (Asia Pacific) Flexible, strong flame-retardant, halogen-free extrusion grade intended for evaluation in applications such as wire insulation and cable jacket. Flame retardant performance capable of meeting UL VW-.. |
|||
Flexural Modulus | 0.150 GPa | 21.8 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DEL22P PC (Asia Pacific) LNP STAT-KON* DEL22P is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Flexural Modulus | 0.150 GPa | 21.8 ksi | ASTM D790 |
UBE PAE1200U Nylon Elastomer Description: UBESTA Nylon 12 ElastomerInformation provided by UBE. |
|||
Flexural Modulus | 0.150 GPa | 21.8 ksi | ASTM D790 |
UBE PAE1200U2 Electronic Grade Nylon Elastomer Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |
|||
Flexural Modulus | 0.150 GPa | 21.8 ksi | ASTM D790 |
Eastman Eastman AP005 Copolyester Applications:Automotive componentsBreathable filmsElectrical/electronic componentsFilm ModificationFlexible hingesHose mandrelIndustrial componentsIndustrial hoses/beltsOffice furniturePackagingPoly.. |
|||
Flexural Modulus | 0.150 GPa | 21.8 ksi | ASTM D790 |
Eastman Eastman AP006 Copolyester Applications:Automotive componentsBreathable filmsElectrical/electronic componentsFilm ModificationFlexible hingesHose mandrelIndustrial componentsIndustrial hoses/beltsOffice furniturePackagingPoly.. |
|||
Flexural Modulus | 0.150 GPa | 21.8 ksi | ASTM D790 |
Eastman Eastman AP007 Copolyester Applications:Automotive componentsBreathable filmsElectronic componentsFilm ModificationFlexible hingesHose mandrelIndustrial componentsOffice furniturePackagingPolymer modificationProfilesRubber an.. |
|||
Flexural Modulus | 0.150 GPa | 21.8 ksi | ASTM D790 |
Eastman Neostar FN005 Elastomer Neostar FN005 elastomer is a tough, clear, durable copolyester ether. It was designed for use in the profile and automotive markets, but is also used in packaging and tubing applications where tough.. |
|||
Flexural Modulus | 0.150 GPa | 21.8 ksi | ASTM D790 |
Eastman Neostar FN006 Elastomer Neostar FN006 elastomer is the second in Eastman’s series of tough, clear, durable copolyester ethers. Developed for use in the profile and automotive markets, it can also be used in packaging and .. |
|||
Flexural Modulus | 0.150 GPa | 21.8 ksi | ASTM D790 |
Eastman Neostar FN007 Elastomer Neostar FN007 elastomer is the third in Eastman’s series of tough, clear, durable copolyester ethers. Though originally designed for use in the profile and automotive markets, this innovative copol.. |
|||
Flexural Modulus | 0.150 GPa | 21.8 ksi | SAE J949 |
Azdel SuperLite® SL552000-100 PP Resin Matrix / 55% Glass Fiber (12 mm Molded Thickness) AZDEL SuperLite® SL552000-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |