Mechanical Properties Metric English Comments
Flexural Modulus 1.42 GPa
206 ksi
Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790
Network Polymers NPP 30-2000
Description: Homopolymer PolypropyleneInformation provided by Network Polymers Inc.
Flexural Modulus 1.42 - 17.9 GPa
206 - 2600 ksi
Average value: 2.49 GPa Grade Count:112
Overview of materials for Polybutylene Terephthalate (PBT), Unreinforced, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Unreinforced, Molded". Each property range of values reported is minim..
Flexural Modulus 1.42 GPa
206 ksi
2mm/min; ASTM D790
3M Dyneon™ PVDF 1012/0180 Polyvinylidene Fluoride  (discontinued **)
Improved clarity and flexibility compared to PVDF 1012/0001Improved impact strengthImproved processing compared to PVDF 1012/0001Improved drawabilityExcellent for filament sizes 6 to 30 milsInformat..
Flexural Modulus 1.42 GPa
206 ksi
ASTM D790
PolyOne Edgetek® NJ-000/000 Nylon 12  (discontinued **)
Description/Features:General Purpose GradeHeat StabilizedHigh FlowUL 94 HBProcessing Method:Injection MoldingPolyOne First ChoiceInformation provided by PolyOne Corporation.
Flexural Modulus 1.42 GPa
206 ksi
ASTM D790
Hyosung Topilene J340E PP
J340E Impact CopolymerApplications:Corrugated sheetThick board (tank, etc…)Characteristics:High impactHigh stiffnessLow warpageInformation provided by Hyosung Corporation
Flexural Modulus 1.42 GPa
206 ksi
ASTM D790
Hyosung Topilene J642 PP
J642 Injection Impact CopolymerApplications:Washing M/C partsElectric applianceCharacteristics:Medium impactHigh stiffnessInformation provided by Hyosung Corporation
Flexural Modulus 1.42 GPa
206 ksi
ASTM D790
Hyosung Topilene S905H PP
S905H Fiber Grade HomopolymerApplications: SpunboundCharacteristics:High flowabilityProcessabilityInformation provided by Hyosung Corporation
Flexural Modulus 1.42 GPa

@Thickness 6.40 mm
206 ksi

@Thickness 0.252 in
10mm/min; ASTM D790
LG Chemical LUPOL TE5109 PP+Rubber+MF, High Impact
Description: Injection Molding, PP+Rubber+MF, High Impact, Good WeatherabilityApplication: Automotive Exterior (Bumper Fascia, Rear Bumper Step)Information provided by LG Chemical
Flexural Modulus 1.42 GPa
206 ksi
1% secant; ASTM D790-02
Ipiranga Petrochem PH 0952 Polypropylene
The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr..
Flexural Modulus 1.42 GPa
206 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics SABIC PPCOMPOUND 8620A PP
SABIC® PPcompound 8620A is a mineral filled, impact modified polypropylene TPO. It was originally designed for painted automotive bumper fascia applications where a combination of good flow, hig..
Flexural Modulus 1.42 GPa
206 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Xenoy® EXXY0113 PBT (Asia Pacific)
Blow Moldable Impact modified XENOYThis data was supplied by SABIC-IP for the Asia Pacific region.
Flexural Modulus 1.42 GPa
206 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Xenoy® EXXY0113 PBT (Europe-Africa-Middle East)
Blow Moldable Impact modified XENOYThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Flexural Modulus 1.42 GPa
206 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Xenoy® X6800BM PBT
Blow moldable, impact modifed XENOYThis data was supplied by SABIC-IP for the Americas region.
Flexural Modulus 1.42 GPa
206 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Xenoy® X6800BM PBT (Asia Pacific)
Blow moldable, impact modifed XENOY
Flexural Modulus 1.42 GPa
206 ksi
ASTM D790
Styron LGF 7600 Polypropylene
Overview: STYRON LGF7600 is intended for use injection molding applications that require high stiffness. The material has good processability and fast cycle times. It contains nucleating agent. LGF ..
Flexural Modulus 1.42 GPa
206 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics NORYL PPX PPX7112 PPE+PP (Europe-Africa-Middle East)
PPE+PP blend. Suitable for painted exterior automotive applications.
Flexural Modulus 1.42 GPa
206 ksi
ASTM D790
SCG Chemicals EL-Proâ„¢ P700J Polypropylene Injection Molding
Key Characteristics:High stiffnessHigh glossHigh productivityGood processabilityOdorlessSafe for food contactRecommended Applications:General purpose housewaresFood containersMedical instrumentsInfa..
Flexural Modulus 1.42 GPa
206 ksi
ASTM D790
SCG Chemicals EL-Proâ„¢ P842J Polypropylene Injection Molding
Key Characteristics:Excellent flowabilityExcellent processabilityExcellent stiffnessSuitable for complex parts and large partsRecommended Applications:Electrical appliance parts, mainly for refriger..
Flexural Modulus 1.42 GPa
206 ksi
ASTM D790
UBE UBESTA® 3014U Rigid Electronic Grade Nylon 12
Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System..
Flexural Modulus 1.42 GPa
206 ksi
ASTM D790
UBE UBESTA® 3024U Rigid Electronic Grade Nylon 12
Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System..
Flexural Modulus 1.42 GPa
206 ksi
Zylog Hipolyene® 8110 Thermoplastic Polyolefin & PP Compound
Information provided by Zylog Plastalloys Pvt. Ltd.
Flexural Modulus 1.42 GPa
206 ksi
ASTM D790
UBE UBESTA® 3030XA Nylon 12 Film
Description: UBESTA Nylon 12 FilmInformation provided by UBE.
Flexural Modulus 1.42 GPa
206 ksi
ASTM D790
UBE UBESTA® 3035UF Rigid Piping Grade Nylon 12
Description: UBESTA contributes to the field of Utilities such as plastic pipe system evolutionary developed for gas industry. It is used for both burial and for rehabilitation of existing cast iron..
Flexural Modulus 1.42 GPa
206 ksi
ASTM D790
Covestro Baydur® SFR-243 Polyurethane Composite RRIM Foam, 15% Milled Glass Filled, MDI-based 2-Component Liquid System
0.25 in. thickness.Information provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – C..
Flexural Modulus 1.42 GPa
206 ksi
SAE J949
Azdel SuperLite® SL550600-100 PP Resin Matrix / 55% Glass Fiber (2 mm Molded Thickness)
AZDEL SuperLite® SL550600-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Flexural Modulus 1.42 GPa
206 ksi
SAE J949
Azdel SuperLite® SL551200-100 PP Resin Matrix / 55% Glass Fiber (3 mm Molded Thickness)
AZDEL SuperLite® SL551200-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Flexural Modulus 1.42 GPa
206 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Xenoy® X6800BM PBT (Europe-Africa-Middle East)
Blow moldable, impact modifed XENOY
Flexural Modulus 1.42 GPa
206 ksi
ASTM D790
UBE UBESTA® P3014U Powder Electronic Grade Nylon 12
Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System..