Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 14.0 GPa | 2030 ksi | STN EN ISO 178 |
Plastcom SLOVAMID 66 GF 50 Polyamide 66, 50% Glass Fiber FeaturesChemically reinforced with 50% glass fiber, suitable for mouldings with high strength and toughness also at low temperatures. Used in the automotive, engineering and electrical industry. W.. |
|||
Flexural Modulus | 14.0 GPa | 2030 ksi | ISO 178 |
PolyOne OnForce™ LFT NN-50LGF/000 HS Natural Polyamide 66 (Nylon 66) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Flexural Modulus | 14.0 GPa @Temperature 23.0 °C |
2030 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB SCANMID 6 B12^ F50 Nylon 6, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Flexural Modulus | 14.0 - 18.0 GPa | 2030 - 2610 ksi | Injection and Compression; ISO 178 |
Raschig Group 3536 Epoxy Glass-fiber reinforced epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. This product meets the allowed.. |
|||
Flexural Modulus | 14.0 GPa | 2030 ksi | ASTM D790 |
LATI LAXTAR G/30 30% Glass Reinforced LCP
(discontinued **) Description: Laxtar products are liquid crystal polymers (LCP). They offer exceptional performance together with increasing cost-effectiveness. Due to the outstanding fluidity at high shear rates LC.. |
|||
Flexural Modulus | 14.0 GPa | 2030 ksi | |
Cookson Group Plaskon® SMT-B-1™ Epoxy Molding Compound for PBGAs
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.An epoxy molding compound optimized specifically for grid arrays (BGA/LGA). It is formulated with a unique resin system that min.. |
|||
Flexural Modulus | 14.0 GPa | 2030 ksi | |
Cookson Group Plaskon® ULS-12HLG Epoxy Encapsulant
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.A state-of-the-art, ultra low stress epoxy encapsulant designed for packaging large, stress-sensitive DIPs, PLCCs and QFPs. It i.. |
|||
Flexural Modulus | 14.0 GPa | 2030 ksi | |
Cookson Group Plaskon® ULS-12 Epoxy Encapsulant
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.A state-of-the-art, ultra low stress epoxy encapsulant designed for packaging large, stress-sensitive DIPs, PLCCs and QFPs. It i.. |
|||
Flexural Modulus | 14.0 GPa | 2030 ksi | |
Cookson Group Plaskon® ULS-12LA Molding Compound
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.An ultra low stress, low alpha emission molding compound designed for packaging stress-sensitive memory devices such as TSOPs and.. |
|||
Flexural Modulus | 14.0 GPa | 2030 ksi | ISO 178 |
DSM Akulon® Ultraflow™ K-FG0 Nylon 6-50% Glass Reinforced (European and Asian Grade) (Dry)
(discontinued **)& The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Flexural Modulus | 14.0 GPa | 2030 ksi | |
Lehmann & Voss LUVOCOM® 1105-8004 PEEK, with carbon fiber, low-warpage, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts.High chemical resistance parts, hydrolysis resi.. |
|||
Flexural Modulus | 14.0 GPa | 2030 ksi | |
Lehmann & Voss LUVOCOM® 1301-8457 PPS, linear, with carbon fiber, lubricant modified Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.Strong, stiff parts.Suitable fo.. |
|||
Flexural Modulus | 14.0 GPa | 2030 ksi | |
Lehmann & Voss LUVOCOM® 19-7319 Polyamide 46, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive.. |
|||
Flexural Modulus | 14.0 GPa | 2030 ksi | |
Lehmann & Voss LUVOCOM® 80-7050 Polyacetal-copolymer, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for.. |
|||
Flexural Modulus | 14.0 GPa | 2030 ksi | ASTM D790 |
Solvay TECHNYLSTARâ„¢ SX 218 V50 BK 38N-K PA6, 50% glass filled, DRY Description: High stiffness materials Technylstar polyamide 6, reinforced with 50% of glass fiber, heat stabilized, for injection molding. Characterized by a high fluidity of the melt.Available in: .. |
|||
Flexural Modulus | 14.0 GPa | 2030 ksi | ISO 178 |
Solvay Specialty Polymers Ryton® R-4-220BL Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4-220NA and R-4-220BL 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength after constant or repeated exposure to high temperature water.Featur.. |
|||
Flexural Modulus | 14.0 GPa | 2030 ksi | ASTM D790 |
Lubrizol Isoplast® 101LGF60BLK Engineering Thermoplastic Polyurethane Resin Available in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Flexural Modulus | 14.0 GPa | 2030 ksi | |
Cosmic Plastics E4940 Mineral & Glass Filled Epoxy Molding Compound, Encapsulated Grade Data provided by the manufacturer. |
|||
Flexural Modulus | 14.0 GPa | 2030 ksi | ISO 178 |
Polyram PlusTek PB302G50BK39D Nylon 6, 50% Glass Fiber Reinforced, UV and Heat Stabilized 50% Glass fiber reinforced, UV and heat stabilized Nylon 6. Approved and listed by W.R.C. Potable Water and NSF/ANSI 61 International.Information provided by Polyram. |
|||
Flexural Modulus | 14.0 GPa | 2030 ksi | |
Cytec Thornel® VCK Carbon Cloth Laminate with Mil R-9299 Resin Data provided by the manufacturer, Amoco Performance Products, Inc.Carbon and graphite cloths, consisting entirely of flexible filaments, are produced by pyrolysis of rayon cloth at high temperature.. |
|||
Flexural Modulus | 14.0 GPa | 2030 ksi | ISO 178 |
CENTROPLAST CENTROMID 6.6 CF 20 Polyamide 6.6 carbon fiber This material has very high strength and a high operating temperature. It can be used for precision components, drive parts and housings.Information provided by CENTROPLAST Engineering Plastics GMB.. |
|||
Flexural Modulus | 14.0 GPa | 2030 ksi | |
Lehmann & Voss LUVOCOM® 1301-8305 PPS, linear, with glass fiber, lubricant modified Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.Improved friction and wear behaviour. Emergency running property.Inherent flam.. |
|||
Flexural Modulus | 14.0 GPa @Temperature 23.0 °C |
2030 ksi @Temperature 73.4 °F |
ISO 178 |
Solvay Specialty Polymers Amodel® HFZ A-1145 L Polyphthalamide (PPA)
(Unverified Data**) Amodel® HFZ A-1145 L is a high-flow, 45% glass-fiber-reinforced grade. - Natural: HFZ A-1145 L NT - Black: HFZ A-1145 L BK 937Information provided by Solvay Specialty Polymers. |