Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 13.8 GPa | 2000 ksi | ASTM D790 |
Oxford Polymers Oxnilon 6-50GF 50% Glass Fiber Filled Nylon 6 for Injection Molding 50% Glass Fiber Filled Nylon 6 for Injection MoldingInformation provided by Oxford Polymers. |
|||
Flexural Modulus | 13.8 GPa | 2000 ksi | ASTM D790 |
Oxford Polymers Oxnilon 66-50GF 50% Glass Fiber Filled Nylon 66 for Injection Molding 50% Glass Fiber Filled Nylon 66 for Injection MoldingInformation provided by Oxford Polymers. |
|||
Flexural Modulus | 13.8 GPa | 2000 ksi | ASTM D790 |
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent creep .. |
|||
Flexural Modulus | 13.8 GPa | 2000 ksi | ASTM D790 |
PolyOne Lubri-Tech™ PK-30CF/15T Polyetheretherketone (PEEK), Carbon Fiber Reinforced, PTFE Lubricated
(discon Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 13.8 GPa | 2000 ksi | ASTM D790 |
Solvay Specialty Polymers Amodel® AS-1145 HS Polyphthalamide (PPA), 45% Glass Fiber (Conditioned) Amodel® AS-1145 HS is a 45% glass reinforced heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater tha.. |
|||
Flexural Modulus | 13.8 GPa | 2000 ksi | ASTM D790 |
Techmer ES Electrafil® J-50/CF/30/TF/13/SI/2 Polycarbonate, 30% Carbon Fiber Reinforced, 13% PTFE, 2% Silicone |
|||
Flexural Modulus | 13.8 GPa | 2000 ksi | ASTM D790 |
Solvay Specialty Polymers Ryton® R-4-240BL Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4-240NA and R-4-240BL 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength and toughness compared to other polyphenylene sulfide compounds.Feat.. |
|||
Flexural Modulus | 13.8 GPa | 2000 ksi | ASTM D790 |
Sumitomo Bakelite North America RX® 643 Fiberglass Reinforced Phenolic RX 643 is a fiberglass reinforced, ammonia-free, phenolic resole compound, with good dimensional stability and good strength at elevated temperatures. Meets ASTM D-5948 Type GPI-10.Information pro.. |
|||
Flexural Modulus | 13.8 GPa | 2000 ksi | ASTM D790 |
Sumitomo Bakelite North America 52-20-30 Short-Glass Reinforced Diallyl Phthalate Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Information provided by Sumitomo Bak North Americ.. |
|||
Flexural Modulus | 13.8 GPa | 2000 ksi | 45° stress angle |
Cytec Cyply® 1002 Epoxy Fiberglass Composite, Unidirectional CYPLY® 1002 is a cured epoxy composite material based on a unique non-woven parallel filament construction. This type of construction minimizes filament stress abrasion that can shorten fatigue li.. |
|||
Flexural Modulus | 13.8 GPa | 2000 ksi | ASTM D790 |
Ashley Polymers Ashlene® 830L-50G Nylon 6, 50% Glass Reinforced Nylon 6, 50% glass reinforced resin.Data provided by the manufacturer |
|||
Flexural Modulus | 13.8 GPa | 2000 ksi | Lengthwise; ASTM D790 |
Bedford Plastics Glass Reinforced FR Polyester Flat Sheet, 3/8" to 1" Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Flexural Modulus | 13.8 GPa | 2000 ksi | Lengthwise; ASTM D790 |
Bedford Plastics Glass Reinforced Vinylester Flat Sheet, 3/8" to 1" Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Flexural Modulus | 13.8 GPa | 2000 ksi | ASTM D790 |
Solvay Specialty Polymers Amodel® AS-1145 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-1145 HS is a 45% glass reinforced heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater than 0... |
|||
Flexural Modulus | 13.8 GPa | 2000 ksi | ASTM D790 |
Techmer ES Electrablend® PA6 E CF20 20% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 20% Filler by WeightFeatures: Conductive Appearance: Natural ColorProcessing Method: ExtrusionInformation p.. |